Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 196 GPa | 28400 ksi | RT |
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Modulus of Elasticity | 196 GPa | 28400 ksi | RT |
Outokumpu 4841 High Temperature Austenitic Stainless Steel Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r.. |
|||
Modulus of Elasticity | 196 GPa | 28400 ksi | RT |
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 300 °C |
28400 ksi @Temperature 572 °F |
|
Haynes 230® alloy, 10% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 300 °C |
28400 ksi @Temperature 572 °F |
|
Haynes 230® alloy, 10% cold reduction, 1177°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 300 °C |
28400 ksi @Temperature 572 °F |
|
Haynes 230® alloy, 30% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 300 °C |
28400 ksi @Temperature 572 °F |
|
Haynes 230® alloy, 40% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 300 °C |
28400 ksi @Temperature 572 °F |
|
Haynes 230® alloy, plate, 1000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, 50% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, SMAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 30% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 9.5 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, plate and bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Modulus of Elasticity | 196 GPa | 28400 ksi | typical of UNS N08800 |
ATI Allegheny Ludlum Type 332 Stainless Steel, UNS N08800 Type 332 is a nickel and chromium austenitic stainless steel designed to resist oxidation and carburization at elevated temperatures. The nickel content, 32%, makes the alloy highly resistant both .. |
|||
Modulus of Elasticity | 196 GPa | 28400 ksi | |
Industeel SIRIUS 800 H Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at tempe.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, GMAW, as welded, notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, GTAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, GTAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 31.8 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 300 °C |
28400 ksi @Temperature 572 °F |
|
Haynes 230® alloy, cold rolled and 1232°C solution annealed sheet Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 204 °C |
28400 ksi @Temperature 399 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, all-weld metal, GTAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |