Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 214® alloy, 10% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 870°C (1600°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 214® alloy, sheet, 32 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 230® alloy plate, 1000 hours exposure at 649°C (1200°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 230® alloy, 10% cold reduction, 1121°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 230® alloy, 20% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 230® alloy, 20% cold reduction, 1121°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 230® alloy, 40% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 540 °C |
25700 ksi @Temperature 1000 °F |
|
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 540 °C |
25700 ksi @Temperature 1000 °F |
|
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 540 °C |
25700 ksi @Temperature 1000 °F |
|
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 540 °C |
25700 ksi @Temperature 1000 °F |
|
Haynes HR-160® alloy, solution annealed sheet Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 214® alloy, 10% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 214® alloy, 30% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, GTAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, transverse, GMAW spray weldment, 23.4 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 230® alloy, GMAW deposit weld metal Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 230® alloy, hot rolled and 1232°C solution annealed plate Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 230® alloy, plate, 1000 hours exposure at 760°C (1400°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, GTAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 230® alloy plate, 16000 hours exposure at 649°C (1200°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 600 °C |
25700 ksi @Temperature 1110 °F |
|
Haynes 230® alloy, cold rolled and 1232°C solution annealed sheet Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
heat-treated at 1121°C (2050°F), rapid quenched, plate |
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |