Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.90 GPa | 276 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PP 1380 PRE-ELEC PP 1380 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity PR.. |
|||
Modulus of Elasticity | 1.90 GPa | 276 ksi | ISO 527 |
GEHR Plastics PP-30PET-F Polypropylene, 30% PET Fiber Reinforced
(discontinued **) Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle... |
|||
Modulus of Elasticity | 1.90 GPa | 276 ksi | DIN 53457 |
Ineos Nova S-6600 High Impact Compact Polystyrene
(discontinued **) High impact polystyrene which is very easy processed in extension and thermoforming processes. Typical applications are packaging of food stuffs like Yot beakers but technical parts and extruded pr.. |
|||
Modulus of Elasticity | 1.90 - 2.06 GPa | 276 - 299 ksi | Average value: 1.98 GPa Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Modulus of Elasticity | 1.90 - 2.20 GPa @Temperature 60.0 - 90.0 °C |
276 - 319 ksi @Temperature 140 - 194 °F |
Average value: 2.05 GPa Grade Count:1 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Modulus of Elasticity | 1.90 - 9.00 GPa @Temperature 50.0 - 200 °C |
276 - 1310 ksi @Temperature 122 - 392 °F |
Average value: 7.30 GPa Grade Count:7 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Modulus of Elasticity | 1.90 GPa | 276 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® G156A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, specialty applications. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now p.. |
|||
Modulus of Elasticity | 1.90 - 9.31 GPa | 276 - 1350 ksi | Average value: 5.50 GPa Grade Count:21 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Modulus of Elasticity | 1.90 GPa | 276 ksi | ASTM D638 |
Spartech Royalite R632M Carbon Black Filled ABS/PVC Resin Data provided by the manufacturer. This static-conductive material is UL®-listed and meets minimum static-decay requirements outlined in MIL-B-1705B and NFPA Code 56A specifications. |
|||
Modulus of Elasticity | 1.90 GPa | 276 ksi | Conditioned; ISO 178 |
Addiplast Addinyl B2 1 Flame Retardant Nylon 6 Flame retardant, halogen freeInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.90 GPa | 276 ksi | DIN EN ISO 527 |
BASF Elastollan R 2005/1 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Modulus of Elasticity | 1.90 GPa | 275 ksi | Machine; ASTM D638 |
Arlon CuClad 217 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 217 uses a low fiberglass/PTFE ratio to provide the lowest dielectric constant and dissipation factor available in fiberglass reinforced PTFE based laminates. Together, these properties offe.. |
|||
Modulus of Elasticity | 1.90 GPa @Temperature 60.0 °C |
276 ksi @Temperature 140 °F |
ISO 899-1 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Modulus of Elasticity | 1.90 GPa | 276 ksi | ISO 178 |
Addiplast Addinyl C2 R Nylon 66/6 High impact resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.90 GPa | 276 ksi | ISO 527-2 |
BASF Ultraform® N2650 Z2 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr.. |
|||
Modulus of Elasticity | 1.90 - 16.0 GPa | 276 - 2320 ksi | Average value: 4.99 GPa Grade Count:57 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Modulus of Elasticity | 1.90 GPa | 276 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |