Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.80 GPa | 261 ksi | 4 mm thick;10.0 mm wide molded rod; ISO 178 |
Premix Thermoplastics PRE-ELEC® ESD 7100 PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject.. |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | 4 mm thick;10.0 mm wide molded rod; ISO 178 |
Premix Thermoplastics PRE-ELEC® ESD 7200 PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj.. |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | 4 mm thick;10.0 mm wide molded rod; ISO 178 |
Premix Thermoplastics PRE-ELEC® PS 1324 PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PS 1326 PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Modulus of Elasticity | 1.80 - 1.80 GPa @Temperature 100 - 100 °C |
261 - 261 ksi @Temperature 212 - 212 °F |
Average value: 1.80 GPa Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Modulus of Elasticity | 1.80 - 35.2 GPa | 261 - 5100 ksi | Average value: 5.72 GPa Grade Count:175 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Modulus of Elasticity | 1.80 - 6.40 GPa | 261 - 928 ksi | Average value: 5.16 GPa Grade Count:14 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Modulus of Elasticity | 1.80 - 11.0 GPa | 261 - 1600 ksi | Average value: 7.95 GPa Grade Count:43 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Modulus of Elasticity | 1.80 GPa @Temperature 20.0 °C |
261 ksi @Temperature 68.0 °F |
|
Micropol Isoplas P651 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | ASTM D638 |
Spartech Royalite R59M Hi-Impact ABS/PVC Resin Data provided by the manufacturer. A unique ABS/PVC resin that meets the flammability standards of many industries and is a cost-effective alternative to standard fire-rated ABS. High rigidity in t.. |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | ISO 527-2 |
Tisan TISLAMID® 66 Impact Modified Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 15MB440 OPP Film Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin .. |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 38DL247 OPP Film Product Description: A super white opaque, high gloss, high yield and highly cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Av.. |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 38DO447 OPP Film Product Description: A super white opaque BOPP film. The Diamex technology allows for super low density and very high yield. Diamex makes it possible to lower the density, without decreasing the mod.. |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | DIN EN ISO 527 |
BASF Elastollan R 2001 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 G30 Nylon 66, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 ZG30 Nylon 66, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.80 GPa | 261 ksi | ASTM D638 |
Plaskolite West Optix® CA-1000 E Impact Modified Acrylic Resin Extrusion Grade Pellets. Excellent blend stock material for impact applications. |
|||
Modulus of Elasticity | 1.80 - 3.00 GPa | 261 - 435 ksi | Average value: 2.34 GPa Grade Count:243 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Modulus of Elasticity | 1.80 - 3.30 GPa | 261 - 479 ksi | Average value: 2.96 GPa Grade Count:19 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Modulus of Elasticity | 1.80 - 2.41 GPa | 261 - 350 ksi | Average value: 2.09 GPa Grade Count:5 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |