Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 2400 MPa @Temperature 23.0 °C |
348000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo.. |
|||
Tensile Creep Modulus, 1 hour | 2400 MPa | 348000 psi | ISO 899-1 |
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage |
|||
Tensile Creep Modulus, 1 hour | 2400 MPa | 348000 psi | Conditioned; ISO 889-1 |
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp |
|||
Tensile Creep Modulus, 1 hour | 2400 MPa | 348000 psi | ISO 899-1 |
Lanxess Pocan® B 1300 000000 PBT PBT, non-reinforced, injection molding, extrusion |
|||
Tensile Creep Modulus, 1 hour | 2400 MPa | 348000 psi | ISO 899-1 |
Lanxess Pocan® B 1305 000000 PBT PBT, non-reinforced, injection molding |
|||
Tensile Creep Modulus, 1 hour | 2400 MPa @Time 3600 sec |
348000 psi @Time 1.00 hour |
ISO 899-1 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring .. |
|||
Tensile Creep Modulus, 1 hour | 2400 MPa @Time 3600 sec |
348000 psi @Time 1.00 hour |
ISO 899-1 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear .. |
|||
Tensile Creep Modulus, 1 hour | 2400 MPa | 348000 psi | |
Ineos ABS NOVODUR® P2T ABS, Injection Grade
(discontinued **) Injection molding grade, very high heat resistance.Applications: Automotive industry, household appliances.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This g.. |