Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | ASTM D1822 |
Westlake Plastics Pomalux® Acetal Copolymer For Medical Applications Medical grade Pomalux is made from acetal copolymer resin which allows machined products the ability to retain dimensional integrity, maintain stability in water and most chemicals at elevated tempe.. |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | ASTM D1822 |
ExxonMobil HDPE AS55-03 High Density Polyethylene Resin Product Description: AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistatic additive. It provides a good balance of stiffness and stress crack resistance.Avail.. |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AB50-003 Blow Molding Resin Product Description: AB50-003 is a blow molding grade high density polyethylene copolymer. This resin has very good stress crack resistance combined with high impact strength and rigidity.Availabili.. |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AL55-003 Blow Molding Resin Product Description: AL55-003 is a blow molding grade high density polyethylene offering a good combination of stiffness and stress crack resistance.Availability: Latin America, North America and So.. |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7147 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as food containers, housewares and lids. Information provided by D.. |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DNDA-8335 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8335 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AF50-003 Blow Molding Resin AProduct Description: AF50-003 is a blow molding high density polyethylene copolymer containing an antistatic additive. It offers very good balance of stress crack resistance, stiffness and impact s.. |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow UNIVAL™ DMDF-6200 NT 7 High Density Polyethylene Resin (HDPE) Excellent extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDF-6200 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipme.. |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | ASTM D-1822 |
Axiall 9113 White 02 Rigid PVC, Molding, White 02 Georgia Gulf 9113 White 02 is a pre-colored white material with outstanding impact strength and processing properties. It is especially suited for packaging charcoal lighter fluid.Information provi.. |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AA50-002 Blow Molding Resin
(discontinued **) AA50-002 is a blow molding grade high density polyethylene. This resin has excellent stress crack resistance combined with high impact strength, rigidity, and melt strength.Information provided by .. |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AM55-003 Blow Molding Resin
(discontinued **) AM55-003 is a blow molding grade high density polyethylene copolymer containing an excellent antistat additive. It provides a good combination of stiffness and stress crack resistance. AM55-003 co.. |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AS55-003 Blow Molding Resin
(discontinued **) AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistat additive. It provides a good balance of stiffness and stress crack resistance.Information provided by Exx.. |
|||
Tensile Impact Strength | 189 kJ/m² | 90.0 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AU55-003 Blow Molding Resin
(discontinued **) AU55-003 is a blow molding grade high density polyethylene containing an excellent antistat additive, offering a good combination of stiffness and stress crack resistance. An enhanced additive pack.. |