Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 147 kJ/m² | 69.9 ft-lb/in² | |
Kraton® D1102 + LDPE blend (6/94) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Tensile Impact Strength | 147 kJ/m² | 69.9 ft-lb/in² | ASTM Data |
Styron CALIBRE™ 5051 15 Polycarbonate, 5% Glass Reinforced CALIBRE® 5051 is a 5% glass reinforced polycarbonate resin containing mold release for optimal processing. CALIBRE 5051 polycarbonate resin exhibits high modulus and excellent dimensional stabili.. |
|||
Tensile Impact Strength | 147 kJ/m² | 69.9 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 5101-15 Polycarbonate Resin Overview: CALIBREâ„¢ 5101 Polycarbonate resin is 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding .. |
|||
Tensile Impact Strength | 147 kJ/m² | 69.9 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL.. |
|||
Tensile Impact Strength | 147 kJ/m² | 69.9 ft-lb/in² | ASTM Data |
Styron CALIBRE™ 7101 15 Polycarbonate, 10% Glass Reinforced CALIBRE® 7101 is a 10% glass reinforced ignition resistant polycarbonate resin equipped with a mold release package for optimal processing. The CALIBRE 7101 resins exhibit a high modules, excepti.. |
|||
Tensile Impact Strength | 147 kJ/m² | 70.0 ft-lb/in² | Type S; ASTM D1822 |
Chase Plastics CP Pryme® N140MGHL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Tensile Impact Strength | 147 kJ/m² | 70.0 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AA60-003 Blow Molding Resin Product Description: AA60-003 is a medium molecular weight distribution high density polyethylene which is characterized by high stiffness, excellent melt uniformity, and chemical inertness.Availabi.. |
|||
Tensile Impact Strength | 147 kJ/m² | 70.0 ft-lb/in² | Compression molded; ASTM D1822, Type S |
Dow 620I Linear Low Density Polyethylene (LDPE) For extruded foam applications Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Tensile Impact Strength | 147 kJ/m² | 70.0 ft-lb/in² | ASTM D-1822 |
Axiall 7020 Rigid PVC, Extrusion Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityF.. |
|||
Tensile Impact Strength | 147 kJ/m² | 70.0 ft-lb/in² | ASTM D-1822 |
Axiall 3027 Rigid PVC, Extrusion Georgia Gulf 3027 is a powder blend designed as a substrate base for coextruded profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |