Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Precision Polymer Engineering Perlast® G75B High Temperature Perfluoroelastomer Perlast® G75B offers a unique blend of excellent chemical resistance, temperature capabilities and mechanical properties, simultaneously extending the operating limits in all three aspects. Perlas.. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | DIN 53504 |
Huntsman IROGRAN® A 95 E 4861 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A95 4861 is a high performance polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN A95E 4861 is part of the HUNTSMAN technical extrusion pro.. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Huntsman IROGRAN® PS 443-201 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11T95P Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T95P is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical p.. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® D16N98UV Thermoplastic Polyurethane Elastomer Pearlthane® D16N98UV is a polyether-based TPU, supplied in form of transparent, colorless pellets, combining high hardness with excellent mechanical properties and good hydrolysis and microbial r.. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.Main Application : Injection MouldingSpecial Features : Excellent mechanica.. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ISO 37 |
Huntsman AVALON® 92 AB Thermoplastic Polyurethane Introduction: AVALON 92 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 92 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1195 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8264 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1295 Polyester Based TPU Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2198 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Lubrizol Estane® 2355-55DE Thermoplastic Polyurethane Type: Pellethane® 2355-55DE is a thermoplastic polyurethane elastomer.Information Provided by The Lubrizol Corporation |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D638 |
ELASTO UK Dryflex® 420501S SBS Based Material, 50D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D638 |
ELASTO UK Dryflex® 422501S SBS Based Material, 50D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.0120 GPa | 1.74 ksi | Aged 1008 Hrs at 150°C in Air |
DuPont Vamac® DHC Ethylene Acrylic Elastomer
(discontinued **) DuPont™ Vamac® DHC is a dipolymer of ethylene and methylacrylate cured using peroxide vulcanization systems. This gum elastomer includes a small amount of processing aid. It has a mild acrylic odo.. |