Wanhua Chemical Wanthane® WHT-2198 Polycaprolactone Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-2198 Polycaprolactone Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
ASTM D2240
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength 32.0 MPa
4640 psi
ASTM D412
Elongation at Break 480 %
480 %
ASTM D412
100% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
300% Modulus 0.0270 GPa
3.92 ksi
ASTM D412
Tear Strength 135 kN/m
770 pli
ASTM D624
Processing Properties Metric English Comments
Processing Temperature 195 - 215 °C
383 - 419 °F