Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00380 GPa | 0.551 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z800 SHF Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00380 GPa | 0.551 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z800 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00380 GPa | 0.551 ksi | TPE-0153 (ASTM D 412) |
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer designed for glazing and sealing applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonat.. |
|||
100% Modulus | 0.00380 GPa | 0.551 ksi | Formulation Example |
TSE Industries Millathane® 66 Millable Polyurethane Rubber Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical .. |
|||
100% Modulus | 0.00380 GPa | 0.551 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4760P Compound FormulationNordel® IP 4760P |
|||
100% Modulus | 0.00380 GPa | 0.551 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770P Dense Extruded Profile FormulationNordel® IP 4770P |
|||
100% Modulus | 0.00380 GPa | 0.551 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770R Dense Extruded Profile FormulationNordel® IP 4770R |
|||
100% Modulus | 0.00380 GPa | 0.551 ksi | Formulation Example |
TSE Industries Millathane® 66 Millable Polyurethane Rubber Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical .. |
|||
100% Modulus | 0.00380 GPa | 0.551 ksi | ASTM D412; ASTM D638 |
Lubrizol Estane® 58280 Thermoplastic Polyurethane Type: Estane® 58280 is a polyether-type thermoplastic polyurethane (TPU) compound.Features: High resiliency compound, with unique physical properties such as low tensile and compression set, high r.. |
|||
100% Modulus | 0.00380 GPa | 0.551 ksi | ISO 37 |
AlphaGary Evoprene™ HP 3730 High Performance Thermoplastic Elastomer Evoprene™ HP is a hydrogenated styrene block copolymer based thermoplastic elastomer. Specially formulated for applications requiring high strength and excellent abrasion resistance, Evoprene™ HP.. |