Mechanical Properties Metric English Comments
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Gouda Vuurvast AK 55 S Dense Refractory Brick
Description: This andalusite based brick is characterized by a low porosity and a good creep resistance (After 24 hours at 1350°C under a load of 0.2 MPa gives between 14th and 24th hour a creep ..
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Gouda Vuurvast AK 70 K Dense Refractory Brick
Description: A high quality andalusite/corundum brick with a mullite bond with a very good volume stability. Also good slag- and thermal shock resistance.Remarks: This data represents average values..
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Gouda Vuurvast AK 70 M Dense Refractory Brick
Description: This mullite brick is characterized by a very good thermal shock resistance, a high resistance against slag penetration and a high strength.Remarks: This data represents average values,..
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Gouda Vuurvast AK 80 B Dense Refractory Brick
Description: A brick made from very pure Guyana bauxite. For applications under severe working conditions such as electric arc furnace roofs.Remarks: This data represents average values, obtained fr..
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Gouda Vuurvast B 1 Sp Dense Refractory Brick
Description: High mechanical strength and very low porosity are typical for this type of brick. Application: transition zone in cement kilns, incinerators, steel ladles.Remarks: This data represents..
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Gouda Vuurvast B Sp Dense Refractory Brick
Description: A very dense brick, high resistance against slag penetration. Application: in rotary kilns (cement) and incinerators.Remarks: This data represents average values, obtained from samples ..
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Gouda Vuurvast AK 65 A Dense Refractory Brick
Description: This andalusite based brick with a very pure mullite bond has a low alkali and iron content. In addition, it has a high creep resistance and is therefore used in applications where load..
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Gouda Vuurvast AK 70 A Dense Refractory Brick
Description: This brick is made of a high quality bauxite. Application: transition zone of rotary cement kiln.Remarks: This data represents average values, obtained from samples that were cut from s..
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Gouda Vuurvast AK 85 M Dense Refractory Brick
Description: A bauxite based brick with a mullite bond. Application: torpedo ladles, electric arc furnace roofs, cement kilns.Remarks: This data represents average values, obtained from samples that..
Compressive Strength 60.0 MPa
8700 psi
ASTM D362
Unitika M1030B PA6, Conditioned
Nano composite nylonInformation provided by Unitika Ltd.
Compressive Strength 60.0 MPa

@Time 360000 sec
8700 psi

@Time 100 hour
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: ..
Compressive Strength 60.0 MPa

@Time 3.60e+7 sec
8700 psi

@Time 10000 hour
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor..
Compressive Strength 60.0 MPa

@Time 360000 sec
8700 psi

@Time 100 hour
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..
Compressive Strength 60.0 - 150 MPa
8700 - 21800 psi
Perpendicular to Plane
Goodfellow Carbon-Carbon Composite
Carbon Fiber - Carbon MatrixInformation provided by Goodfellow.
Compressive Strength >= 60.0 MPa
>= 8700 psi
Axial; IEC 1212-2 4.2
Hippe EP MP 21 Mica Paper Reinforced Epoxy Resin - Round, Rolled Tube
Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity. Good heat resistance.Information provided by Hippe.
Copyright © lookpolymers.com All Rights Reserved