Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 75.8 MPa | 11000 psi | Break; TM R050-38 |
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Compressive Strength | 76.0 MPa | 11000 psi | |
Pyrotek F-24 Dense Machinable Board F-24 is a high temperature resin material that is reinforced with fiberglass. Abrasion resistant, it is used for hot glass handling applications.ApplicationsDonut rollers for glass Guide rails Wear.. |
|||
Compressive Strength | 75.84 - 103.4 MPa | 11000 - 15000 psi | after 816°C |
Pyrotek Pyrocast ZG Refractory Shapes Aggregate Base: FireclayApplicationsDoor sill Door lintel Door jamb Information provided by Pyrotek. |
|||
Compressive Strength | 76.0 MPa | 11000 psi | 20% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 1200 Cast Polyamide 12, Dry Application: sprockets, chain-wheels, pulleys, wheels, slide and seal rings, curve disks, etc.Information provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 76.0 MPa | 11000 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Compressive Strength | 76.0 MPa @Time 36.0 sec |
11000 psi @Time 0.0100 hour |
|
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis.. |
|||
Compressive Strength | 76.0 MPa | 11000 psi | Longitudinal |
Goodfellow Polyaramid/Polyphenylene Sulfide Composite Sheet or Rod 25% Polyaramid fiber - PPS Matrix. Information provided by Goodfellow. |
|||
Compressive Strength | 75.8 MPa | 11000 psi | Crushing |
Zircar Ceramics DAHP Dense Alumina Hearth Plate ZIRCAR Dense Alumina Hearth Plates are used for supporting loads in high temperature furnaces and other thermal process systems. These dense plates are made of fully sintered fine grain high purity .. |
|||
Compressive Strength | 75.84 MPa | 11000 psi | Service Pressure |
Trelleborg AEM Eccofloat® EL-36/7300 Syntactic Foam EL Grade epoxy syntactic foams are the material of choice for manufacturing manned and unmanned submersibles because of their density range and ability to withstand exposure to diesel fuels and hydr.. |
|||
Compressive Strength | >= 75.8 MPa | >= 11000 psi | |
Master Bond EP41S Fast Curing Epoxy Features Chemical Resistance Description: Master Bond EP41S is a two component epoxy resin compound for durable, high performance, tough, high strength coatings, liners and sealants with outstanding resistance to organic solven.. |
|||
Compressive Strength | 75.8 - 86.2 MPa | 11000 - 12500 psi | ASTM D695 |
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |
|||
Compressive Strength | 75.8 - 103 MPa | 11000 - 15000 psi | |
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame.. |
|||
Compressive Strength | 75.8 MPa | 11000 psi | |
BCC Products BC 7062-3H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |
|||
Compressive Strength | 75.8 - 82.7 MPa | 11000 - 12000 psi | |
Abatron AboCast 7802-1/AboCure 50-12 Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-12 is a clear converter for high rigidity, chemical, and temperature resistance (HDT: 101.. |
|||
Compressive Strength | 75.8 MPa | 11000 psi | Break; TM R050-38 |
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |