Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 112 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 112 MPa
16200 psi
ASTM D695
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula..
Compressive Strength 112 MPa
16200 psi
Perpendicular
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..
Compressive Strength 112 MPa
16200 psi
ASTM D695
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava..
Compressive Strength 112 MPa
16200 psi
ASTM D695
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for..
Compressive Strength 112 MPa
16200 psi
break; DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre..
Compressive Strength 112 MPa
16200 psi
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System
TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and ..
Compressive Strength 112 MPa
16200 psi
ASTM D695
Ensinger Hydel® PEI-7 Polyetherimide (PEI), Static Dissipative
A static dissipative polyetherimide utilizing proprietary filler technology which renders this material electrically conductive. This technology allows for good dimensional stability after machinin..
Compressive Strength 112 MPa
16200 psi
ASTM D695
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir..
Copyright © lookpolymers.com All Rights Reserved