Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 59.0 MPa | 8560 psi | ASTM D638 |
Kolon KOPA® KN333HFBL General Purpose Nylon 66 Middle viscosity, flexibleApplications Band cables for vehiclesInformation provided by API-Kolon. |
|||
Tensile Strength | 59.0 MPa | 8560 psi | ASTM D638 |
Kolon KOPA® KN333HI5BL High Impact Nylon 66 Middle viscosity, Impact -resistantApplications A variety of fuse boxes, relax boxesInformation provided by API-Kolon. |
|||
Tensile Strength | 59.0 MPa | 8560 psi | ASTM D638 |
Kolon KOPA® KN333NW High Impact Nylon 66 Impact -resistant, dimensional safetyApplications Wheel coversInformation provided by API-Kolon. |
|||
Tensile Strength | 59.0 MPa | 8560 psi | ASTM D638 |
Kolon SPESIN® KP513MT25 G/F Reinforced PBT Alloy Resin High flow, dimensionally stableApplications: Head lamp bezelsInformation provided by API-Kolon. |
|||
Tensile Strength | 59.0 MPa | 8560 psi | ISO 527 |
Lucite International Diakon® CRG800 Acrylic Polymer, Toughened Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Tensile Strength | 59.0 MPa | 8560 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPH303G20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH303G20 is a 20% glass filled Polypropylene - Homopolymer injection molding grade with good stiffness.Information provided by SAX Polymers |