Mechanical Properties Metric English Comments
Tensile Strength 34.5 MPa
5000 psi
ASTM D638
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet)
Tensile Strength 34.5 MPa
5000 psi
ASTM D638
Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet)
Tensile Strength 34.5 MPa
5000 psi
ASTM D412
Parker Chomerics CHO-THERM® 1646 Non-Insulating Interface Material
Description: CHO-THERM® 1646 pads offer the best available thermal performance, without the use of grease, in applications where electrical isolation is not required. The low thermal impedance of C..
Tensile Strength 34.5 - 41.4 MPa
5000 - 6000 psi
ASTM D638
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Tensile Strength 34.5 - 55.2 MPa
5000 - 8000 psi
ASTM D638
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Tensile Strength 34.5 - 41.4 MPa
5000 - 6000 psi
ASTM D638
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Tensile Strength 34.5 - 44.8 MPa
5000 - 6500 psi
ASTM D638
Mar-Bal MB4000 Thermoset Polyester Composite Molding Compound
The high track resistant material. A flame retardant polyester molding compound with moderate strength and excellent electrical properties and exceptional arc and track resistance. Suitable for repl..
Tensile Strength 34.5 MPa
5000 psi
ASTM D1708
Garlock GYLON® 3522 PTFE Diaphragm
GYLON PTFE diaphragmWithstands aggressive chemicals and temperatures up to +500°F (+260°C).Up to four times the flex life of conventional PTFEReduced void content - less permeation, increased ..
Tensile Strength 34.5 MPa
5000 psi
across grain; ASTM F152
Garlock GYLON® HP3560 PTFE Gasketing, Steel Insert
Gylon® with perforated 316LSS insertPerforated stainless steel core increases resistance to pressure fluctuations and thermal cyclingGYLON® offers superior cold flow and creep resistance, elim..
Tensile Strength 34.5 MPa
5000 psi
across grain; ASTM F152
Garlock GYLON® HP3561 PTFE Gasketing, Steel Insert
Gylon® with perforated 316LSS insertPerforated stainless steel core increases resistance to pressure fluctuations and thermal cyclingGYLON® offers superior cold flow and creep resistance, elim..
Tensile Strength 34.5 MPa
5000 psi
across grain; ASTM F152
Garlock GYLON® HP3563 PTFE Gasketing, Steel Insert, Oxygen Service
Gylon® with perforated 316LSS insert - Oxygen servicePerforated stainless steel core increases resistance to pressure fluctuations and thermal cyclingGYLON® offers superior cold flow and creep..
Tensile Strength 34.5 - 48.3 MPa
5000 - 7000 psi
Michelman® Hydrosize® U2-01 Nonionic polyurethane emulsion
Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2-01 is a high strength sizing for glass and carbon chopped fiber with excellent adhesion.Information provided by Michelman®
Tensile Strength 34.5 - 48.3 MPa
5000 - 7000 psi
Michelman® Hydrosize® U2022 Nonionic polyurethane emulsion
Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2022 is an APE free, high strength sizing for glass and carbon chopped fiber, with excellent adhesion.Information provided by Michelm..
Tensile Strength >= 34.5 MPa
>= 5000 psi
Measured on solution cast film from toluene; BAM 1245
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Description: Kraton A1536 H is a linear triblock copolymer based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified: Kraton A1536 HU - supplied to cu..
Tensile Strength 34.5 MPa
5000 psi
Typical properties of film cast from toluene solution; ASTM D412
Kraton® FG1901 G (SEBS) grafted with MA
Description: Kraton FG1901 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form id..
Tensile Strength 34.5 MPa
5000 psi
ASTM D412
Kraton® G1650 M (SEBS) Linear Triblock Copolymer
Description: Kraton G1650 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide..
Tensile Strength 34.5 MPa
5000 psi
across grain; ASTM F152
Garlock GYLON® HP3562 PTFE Gasketing, Steel Insert, Oxygen Service
Gylon® with perforated 316LSS insert - Oxygen servicePerforated stainless steel core increases resistance to pressure fluctuations and thermal cyclingGYLON® offers superior cold flow and creep..
Tensile Strength 34.5 MPa
5000 psi
Typical properties of film cast from toluene solution; ASTM D412
Kraton® FG1901 G (SEBS) grafted with MA
Description: Kraton FG1924 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form i..
Tensile Strength 34.5 MPa
5000 psi
ASTM D638, ASTM D1708
ScanTube PVDF Tubing
Information provided by ScanTube, Inc.
Tensile Strength 34.5 MPa

@Temperature 23.9 °C
5000 psi

@Temperature 75.0 °F
Master Bond MB250NT Low viscosity ethyl cyanoacrylate
Master Bond MB250NT is a single component ethyl cyanoacrylate type system. This rapid curing, high strength system is used primarily in applications where the ISO 10993-5 for low toxicity is specifi..
Tensile Strength 34.5 MPa
5000 psi
ASTM D412
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane
Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf..
Tensile Strength >= 34.5 MPa
>= 5000 psi
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy
Master Bond Polymer System EP30LTE-LO is a thermal shock resistant epoxy resin system with low thermal expansion properties and dimensional stability for high performance bonding, sealing and castin..
Tensile Strength >= 34.5 MPa
>= 5000 psi
Master Bond UV15DC80 One Component, UV and Heat Curable Epoxy System
Master Bond UV15DC80 is a special dual cure epoxy based system which offers a primary cure utilizing UV light along with a secondary heat curing mechanism. This system addresses the problem of curin..
Tensile Strength 34.5 MPa
5000 psi
ASTM D638
Ecomass® 1050ZD96 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade
High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and ..
Tensile Strength 34.5 MPa
5000 psi
2 in/min; ASTM D638
Braskem FF026M Homopolymer Polypropylene
Description: Excellent Color and Processing Stability, Superior Optical and Mechanical Properties, Broad Processing WindowApplications: Suggested Uses Include BOPP ApplicationsThis resin meets the r..
Tensile Strength 34.5 MPa
5000 psi
ASTM D412/D638
Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane
Features: It is especially well suited for dispersing co-ferrite as well as Cr02 pigments used in video, audio, and data storage applications. This product offers excellent hydrolytic stability unde..
Tensile Strength 34.5 MPa
5000 psi
Henkel Hysol EA 9320NA Paste Adhesive System
High shear and high peel adhesive system with room temperature cure.
Tensile Strength 34.5 MPa
5000 psi
Henkel SynCore HC 9875 Syntactic Film
High crush strength, low density syntactic core material, co-curable with a variety of 350°F / 177°C curing epoxy prepregs.