Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 20.7 MPa | 3000 psi | |
Ohio Carbon Blank OCB UT-3 Mechanical Grade Graphite Available in a range of sizes and shapes. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-1046LF PVC Compound Application: A 105°C, lead free, tri-rated semi-rigid insulation compound suitable for UL style 1061, CSA-SR-PVC, MIL-I-16878.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 20.7 MPa | 3000 psi | ASTM D638 |
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet) |
|||
Tensile Strength | 20.7 MPa | 3000 psi | Optimum; With provided formulation; ASTM D638 |
PolyOne Geon™ 180 Series 186A Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 186A is low molecular weight homopolymer resin, providing a good balance of fused film physical properties and fusion characteristics. It provides excellent chemical foam characteristics with.. |
|||
Tensile Strength | 20.7 MPa @Strain 100 % |
3000 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 1351 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | >= 20.7 MPa | >= 3000 psi | |
Garlock 135 Natural Sheet Rubber Garlock Natural Rubber Sheet is manufactured from Food and Drug Administration-approved ingredients. It is a superior, long-life sheet designed specifically for general gasketing, countertops and sk.. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | Typical |
Garlock Viblonâ„¢ 276 Neoprene Bearing Pad Viblonâ„¢ pads are technically engineered and specifically designed to cushion impact, shock and vibration. Constructed of multiple layers of high-quality, cotton-polyester duck fabric, completel.. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | ASTM D412 |
Kraton® D1133 K (SBS) Linear Block Copolymer Description: Kraton D1133 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 36%. It is supplied from North America in the physical form identified.. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | Estimated value; ASTM D412 |
Kraton® D1133 K (SBS) Linear Triblock Copolymer Description: Kraton D1133 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 36%. It is supplied from North America in the physical form identified.. |
|||
Tensile Strength | >= 20.7 MPa | >= 3000 psi | Grade A |
Shandong Dongyue Polymer DF-201 PTFE Fine Powder Usage: It is suitable for making unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse.. |
|||
Tensile Strength | >= 20.7 MPa | >= 3000 psi | Grade A |
Shandong Dongyue Polymer DF-202 PTFE Fine Powder Usage: It is mainly used to process, belt, thin sheet and unsintered tape, thin wall rod etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF.. |
|||
Tensile Strength | >= 20.7 MPa | >= 3000 psi | Qualified |
Shandong Dongyue Polymer DF-203 PTFE Fine Powder Usage: The resin is used to process capillary tube, thin-wall tube, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside... |
|||
Tensile Strength | 20.7 MPa | 3000 psi | ASTM D4894 |
Saint-Gobain Fluoroloy® A16 High Performance Seal Material General purpose material for heat and wear resistance; Recommended for dry and poorly lubricated applications; Particularly suitable for water and steam service
Information provided by Saint-Goba.. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | ASTM D638 |
Saint-Gobain Rulon® 945 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Tensile Strength | >= 20.7 MPa | >= 3000 psi | Qualified |
Shandong Dongyue Polymer DF-205 PTFE Fine Powder Usage: The resin is used to process two-side draw film, capillary tube, thin-wall tube, sheet, small-diameter rod, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC ba.. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | ASTM D638 |
Techmer ES HiFill FR® PP CO E FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant and CopolymerProcessing Method: ExtrudedInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | ASTM D638 |
Techmer ES HiFill FR® PP CO FR HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and CopolymerUL File Number: E157318Processing Method: Injection MoldingInformation provi.. |
|||
Tensile Strength | >= 20.7 MPa | >= 3000 psi | |
Master Bond EP21FRNS-2 Two Component, Flame Resistant Epoxy System Master Bond Polymer System EP21FRNS-2 is a two component, room temperature curing, flame retardant compound for potting, encapsulating and casting. Particularly noteworthy are its low smoke generati.. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | ASTM D638 |
Ecomass® 4703BI62 Filled Polyurethane, Injection Molding Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, radiation shielding applicationsInfor.. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | 2 in/min; ASTM D638 |
Braskem TI6800WV Impact Copolymer Polypropylene Description: High Melt Flow, Nucleated, Excellent Mold Release, AntistaticApplications: Suggested Uses Include Housewares, Large Part Injection Molding, Thin-Walled Injection MoldingThis resin meets.. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | |
AlphaGary PVC 7762 Polyvinyl Chloride Thermoplastic Extrusion moldings for exterior parts |
|||
Tensile Strength | 20.7 MPa | 3000 psi | ASTM D638 |
Americas Styrenics EB6400 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | ASTM D638 |
Aaron Industries AVPE LLD 300-2 Virgin Polyethylene Melt flow index may be specified. |
|||
Tensile Strength | 20.7 MPa | 3000 psi | |
AlphaGary GW 2038 VW1 LCF Flame Retardant Polyvinyl Chloride 60°C or 75°C rated jacketing compound for CMR cable per UL 444 |
|||
Tensile Strength | 20.7 MPa | 3000 psi | 2 in/min; ASTM D638 |
Braskem TI6500WV High Impact Copolymer Polypropylene Description: High melt flow, superior low temperature impact, nucleated, good mold release, antistatic.Applications: Suggested uses include compounding, furniture, toys, packaging, large part inject.. |