Material Notes:
Description: Kraton D1133 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 36%. It is supplied from North America in the physical form identified: Kraton D1133 KT - supplied as a dusted porous pelletKraton D1133 KIM - supplied as a dusted powderRegion: Asia Pacific, Europe, Japan, North America, and South America Uses: Kraton D1133 K is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D4025
Volatiles <= 1.0 %
<= 1.0 %
KM 04
Brookfield Viscosity 3500 - 4900 cP

@Temperature 25.0 °C
3500 - 4900 cP

@Temperature 77.0 °F
25% Toluene solution; BAM 922
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Ash 0.15 - 0.35 %
0.15 - 0.35 %
BAM 908
4.0 - 6.0 %
4.0 - 6.0 %
BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
10 seconds. Typical values on polymer compression molded at 150°C (300°F).; ASTM D2240
Tensile Strength 20.7 MPa
3000 psi
ASTM D412
Elongation at Break 800 %
800 %
ASTM D412
300% Modulus 0.00207 GPa
0.300 ksi
ASTM D412
Chemical Properties Metric English Comments
Diblock Content 34 %
34 %
Descriptive Properties Value Comments
Content Antioxidant
0.15-0.40%, KM 08
Polystyrene
34-36%, KM 03
Total Extractables
<1.6%, KM 05
Styrene/Rubber Ratio 36/64