Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Quadrant EPP Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire PEEK is produced to the .. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | 51 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and .. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standa.. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet) |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU)
(Unverified Data**) Udel GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi.. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK) KetaSpire® KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire® PEEK is produced.. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK) KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa.. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK) KetaSpire® KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industr.. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU), Glass Fiber Udel® GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Ensinger XP-132 Compression Molded PI Compound, 15% Graphite Filled The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability.. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D882 |
Arlon 25FR Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Aaron Industries AAROPRENE® G/MFN 6602 Glass and Mineral Filled Nylon 6/6 AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified. |
|||
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Quantum PEEK Information provided by Quantum Advanced Engineering Plastics |