Polymer Property : Tensile Strength = 51.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 51.0 MPa
7400 psi
ASTM D638
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet)
Tensile Strength 51.0 MPa
7400 psi
DAM; ASTM D638
DuPont Performance Polymers Elvamide® 8061 Nylon  (Unverified Data**)
Polyamide MultipolymerInformation provided by DuPont Performance Polymers
Tensile Strength 51.0 MPa
7400 psi
ASTM D638
Ensinger Tecatron® XP-64B Compression Molded PPS Compound, 40% Fiberglass, Black Pigmented
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Tensile Strength 51.0 MPa
7400 psi
ASTM D638
Americas Styrenics MB3150 High Heat Crystal Polystyrene
Product CharacteristicsFast cycling due to high heat distortion temperatureHigh vicat softening temperatureExcellent clarity with slight blue tintGood toughnessFood Contact CompliantUL Classificatio..
Tensile Strength 51.0 MPa
7400 psi
ASTM D638
Aaron Industries AAROPRENE® GFPP 2030 Glass Filled Polypropylene
AAROPRENE® GFPP 2000 Series Glass Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Tensile Strength 51.0 MPa
7400 psi
Cross; IPC TM-650 2.4.18.3
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply
Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal ..
Tensile Strength 51.0 MPa
7400 psi
ASTM D638
Techmer ES HiFill FR® PBT FR-C
Availability: North AmericaForms: PelletsFeatures: Flame RetardantUL File Number: E157318Processing Method: Injection MoldingInformation provided by TP Composites, Inc.