Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 30.0 MPa | 4350 psi | ASTM D638 |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ASTM D638 |
Premix Premi-Glas® 2203-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ASTM D638 |
Premix Premi-Glas® 2203-15 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-15 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ASTM D638 |
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Tensile Strength | 30.0 - 50.0 MPa | 4350 - 7250 psi | ISO 527 |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Tensile Strength | 30.0 - 50.0 MPa | 4350 - 7250 psi | ISO 527 |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | DIN 53288 |
Permabond TA437 Toughened Acrylic Adhesive PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | DIN 53288 |
Permabond TA4246 Toughened Acrylic Adhesive PERMABOND® TA4246 is a 2-part, no-mix, room temperature curing structural adhesive. It is ideal for use on a wide variety of substrate materials and forms a very high strength structural bond with .. |
|||
Tensile Strength | >= 30.0 MPa | >= 4350 psi | ASTM D638 |
Guarniflon PFA Perfluoroalkoxy Polymer Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for appli.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ISO 527 |
Lucite International Elvakon® 4461 Medium Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1180 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-7180 Polycaprolactone Based TPU Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8264 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ASTM D638 |
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ASTM D638 |
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ISO 37 |
BASF Elastollan 1154 D FHF TPUR Flame Retardant Halogen Free Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan 1185 A M TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan 1185 A W TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 30.0 MPa @Strain 300 % |
4350 psi @Strain 300 % |
ISO 37 |
BASF Elastollan B 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 30.0 MPa @Strain 300 % |
4350 psi @Strain 300 % |
ISO 37 |
BASF Elastollan C 59 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 30.0 MPa @Strain 2.00 %, Temperature 60.0 °C |
4350 psi @Strain 2.00 %, Temperature 140 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 3000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ISO 527 |
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan C 70 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | 50 mm/min; ISO 37 |
BASF Elastollan R 1001 10% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 30.0 MPa @Strain 100 % |
4350 psi @Strain 100 % |
ISO 37 |
BASF Elastollan S 74 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1585 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ISO 37 |
BASF Elastollan S 60 AWH TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 30.0 MPa | 4350 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1570 Polyester Based TPU Plasticizer free, excellent abrasion & slip resistance, low temperature flexibility, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 30.0 - 39.0 MPa | 4350 - 5660 psi | ISO 527 |
BASF Ecovio® C2203 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |