Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 18.0 MPa | 2610 psi | ISO 527 |
S&E Specialty Polymers TufFill™ 5003UV Polyolefin Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p.. |
|||
Tensile Strength | 18.0 MPa | 2610 psi | ISO 527 |
S&E Specialty Polymers TufFill™ 5004UV Polyolefin Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p.. |
|||
Tensile Strength | >= 18.0 MPa | >= 2610 psi | DIN 53504 |
NEXA® PFX8010 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
Tensile Strength | >= 18.0 MPa | >= 2610 psi | DIN 53504 |
NEXA® PFX8012 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
Tensile Strength | >= 18.0 MPa | >= 2610 psi | DIN 53504 |
NEXA® PFX8034 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
Tensile Strength | 18.0 MPa | 2610 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi.. |
|||
Tensile Strength | 18.0 MPa | 2610 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Tensile Strength | 18.0 MPa | 2610 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data) Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The.. |
|||
Tensile Strength | 18.0 MPa | 2610 psi | ASTM D412 |
GRECO ISOTHANE 1680AE Polyether TPU Resin ISOTHANE 1600 series products are polyether based thermoplastic polyurethanes with good balanced qualities. They exhibit high moisture vapor transmission. The product can be e xtruded and blowed.Inf.. |
|||
Tensile Strength | 18.0 - 23.0 MPa | 2610 - 3340 psi | ASTM D4894 |
Isoflon PTFE + 15% Ceramic Polytetrafluoroethylene with 15% Ceramic Properties:Improved compression resistanceGood dielectric characteristicsGood thermal insulationMachining can be trickyApplications: Electrical applicationsInformation provided by Isoflon. |
|||
Tensile Strength | 18.0 - 23.0 MPa | 2610 - 3340 psi | ASTM D4894 |
Isoflon PTFE + 15% Graphite Polytetrafluoroethylene with 15% Graphite Properties:Good thermal conductivityLow coefficient of frictionLow permeabilityApplications: Non-lubricated dynamic seals.Information provided by Isoflon. |
|||
Tensile Strength | 18.0 MPa | 2610 psi | ISO 527 |
MRC Polymers MAXTEL™ 620-BK Polypropylene Copolymer • For injection molding• Excellent process ability with high flow and high impact.Information provided by MRC Polymers Inc. |
|||
Tensile Strength | 18.0 MPa | 2610 psi | DIN 53504 |
Vicone High Performance Rubber VicoSeal™ 07EK-BK High Performance EPDM Rubber Peroxide Cured |
|||
Tensile Strength | 18.0 MPa | 2610 psi | ASTM D638 |
DuPont™ HPF® 1000 Amorphous Polymer for Golf Balls DuPont™ HPF 1000 is extremely versatile and can be used to manufacture all layers of golf balls. DuPont™ HPF 1000 offers a combination of high resilience and low compression. This polymer is a hig.. |
|||
Tensile Strength | >= 18.0 MPa | >= 2610 psi | ISO 37 |
Austin Novel Materials Texalan® 265A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Strength | >= 18.0 MPa | >= 2610 psi | ISO 37 |
Austin Novel Materials Texalan® 765A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tensile Strength | >= 18.0 MPa | >= 2610 psi | ISO 37 |
Austin Novel Materials Texalan® 570A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Strength | 18.0 MPa @Strain 100 % |
2610 psi @Strain 100 % |
ISO 37 |
BASF Elastollan S 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | >= 18.0 MPa | >= 2610 psi | extruded; ASTM D1708 |
Guarniflon PTFE G300 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |