Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 11 g/10 min @Load 21.6 kg, Temperature 190 °C |
11 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Polymer Industries Densetec HDPE Pipe Grade The material displays improved performance characteristics in a variety of piping applications. In addition the material is UV stabilized and ideal for use in demanding outdoor applications. It reta.. |
|||
High Load Melt Index | 11 g/10 min @Load 21.6 kg, Temperature 190 °C |
11 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Novapol® HE-W959-A HDPE Extrusion/Blow Molding Resin HE-W959-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
High Load Melt Index | 11 g/10 min @Load 21.6 kg, Temperature 190 °C |
11 g/10 min @Load 47.6 lb, Temperature 374 °F |
High Load; ASTM D1238 |
Chevron Phillips HiD® 9396T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by.. |
|||
High Load Melt Index | 11 g/10 min @Load 21.6 kg, Temperature 190 °C |
11 g/10 min @Load 47.6 lb, Temperature 374 °F |
High Load; ASTM D1238 |
Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by.. |
|||
High Load Melt Index | 11 g/10 min @Load 21.6 kg |
11 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
High Load Melt Index | 11 g/10 min | 11 g/10 min | ASTM D1238 |
Formosa Plastics Formolene® E905 Film HDPE
(discontinued **) HMW-Bimodal ResinApplications: T-shirt bags, trash can liners, heavy duty bagsFormolene E905 is a high molecular weight grade of HDPE with well-balanced strength in both the machine (MD) and transve.. |
|||
High Load Melt Index | 11 g/10 min @Load 21.6 kg, Temperature 190 °C |
11 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Braskem BS 002J HDPE Blow Molding Polyethylene
(discontinued **) Applications: Bottles up to 60 liters with high ESCR; bottles for surface-active agents. Information provided by Braskem |
|||
High Load Melt Index | 11 g/10 min @Load 21.6 kg, Temperature 190 °C |
11 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE82085 BLUE MASTERBATCH BLUE PE82085 is a blue LDPE based masterbatch containing 30% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Blue 15:1.Method of Usage: BLUE PE82085 is designed fo.. |
|||
High Load Melt Index | 11 g/10 min @Load 21.6 kg |
11 g/10 min @Load 47.6 lb |
ISO 1133 |
SIDPEC EGYPTENE® HD 5301 EA HDPE Blow Molding Applications:High performance blow molded containers typically of to 60 liters capacity for packaging aggressive productsRobust industrial and technical moldingsInformation provided by Interchim s.r.. |
|||
High Load Melt Index | 11 g/10 min @Load 21.6 kg |
11 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total 2285 HDPE Bimodal Film Resin Applications: T-shirt sacks, trash can liners, merchandise bags, multi-wall liner, deli wrapInformation provided provided by Total Petrochemicals. |
|||
High Load Melt Index | 11 g/10 min @Load 21.6 kg, Temperature 190 °C |
11 g/10 min @Load 47.6 lb, Temperature 374 °F |
Condition F; ASTM D1238 |
Formosa Plastics Formolene® E925 Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E925 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics.. |
|||
High Load Melt Index | 11 g/10 min @Load 21.6 kg, Temperature 250 °C |
11 g/10 min @Load 47.6 lb, Temperature 482 °F |
|
BASF Luranyl® KR 2403 G4 Polyphenylene Ether + Styrene-Butadiene Blend, 20% Glass Fiber Reinforced General-purpose grade with 20% glass fiber for parts requiring especially good resistance to heat deformation.Applications: sanitary fittings and parts for fans, computer keyboards.Data was collecte.. |
|||
High Load Melt Index | 11 g/10 min @Load 21.6 kg |
11 g/10 min @Load 47.6 lb |
ISO 1133 |
Total Lacqtene® 2001 TN 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TN 46 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2001 TN 46 is used for sewage pipe, smooth protective condu.. |