Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.5% retained |
Imerys Aftonâ„¢ R Kaolin Afton is a fine-grained kaolin used asa a filler in hard rubber products, plastic products, adhesives, protective coatings and similar applications.Information provided by Imerys |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.5% retained |
Imerys Allenâ„¢ R Kaolin Allen is an intermediate-grained kaolin suitable for use as a filler in soft rubber products, plastic compounds, adhesives, protective coatings and similar applications.Information provided by Imery.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.5% retained |
Imerys Franklin™ R Kaolin Franklin R is an intermediate-grained Kaolin used as a filler is “soft†rubber products, plastic compounds, adhesives, protective coatings and similar applications.Information provided by .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.1% retained |
Imerys Hydrated Aluminum Silicate KT 90A-1 Kaolin KT 90A-1 is a Hydraetd Aluminum Silicate. It is a high surface area, fine particle size clay that is well suited for use as an econoMical filler.Information provided by Imerys |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 2.5% retained |
Imerys Kingsleyâ„¢ Kaolin Kingsley is a coarse-grained, white firing kaolin used in the dinnerware, tile, artware and electrical porcelain industries.Information provided by Imerys |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 3.5% retained |
Imerys KT Cast Slurryâ„¢ Kaolin KT Cast Slurry is a carefully controlled kaolin-water suspension formulated for use in ceramic operations.Information provided by Imerys |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.005% Retained |
KaMin Hydraprint® Kaolin Clay - Filler Hydraprint® kaolin clay is a standard delaminated filler for paper applications. Industry: PAPER & PACKAGINGUses: Coated 1S Label, Coated Bleached Board, Coated Recycled Board, Coated Natural Kra.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.005% Retained |
KaMin KaMin® 90B Kaolin Clay - Waterwashed KaMin® 90B is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90B is ideally suited for water-borne applications where high gloss, holdout and .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | Powder |
Lucas-Milhaupt Lucanex 716 Active Metal Brazing Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.005% Retained |
KaMin Polyfil® XB Kaolin Clay - Waterwashed Cost effective, kaolin extender offering improved consistency vs air floated clays, spray-dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & CableIn.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
Silberline 4-Allâ„¢ E 3266AR The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a pr.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.1% retained |
Silberline Aquasil® "BP" 5745 Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 1% retained |
Silberline Aquasil® "BP" SN Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
Silberline Sparkle Silver Ultraâ„¢ 6756 Sparkle Silver Ultraâ„¢ grades are very bright lenticular automotive aluminum pigments. They offer a very smooth patina and narrow particle size distribution, allowing the formulator to create ve.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 1% retained |
Silberline Stamford "P" Stamford P is a standard polished grade; class "B", medium sized, leafing aluminum pigment carried in mineral spirits.Applications: Trade & Maintenance |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 5% retained |
Silberline Sparkle Silver® 3666 Sparkle Silver® 3666 is a coarse, bright, regular purity, non-leafing aluminum pigment popular for solvent-based general industrial coatings. This pigment can be used with tints to produce a wide.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
Silberline Tufflake® 3700 Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 84% Passes |
Excalibar ExCal® CW 200 Calcium Carbonate CaCO3 Powder ExCal® CW calcium carbonate products are processed from a high-purity ore, to exacting specifications at the Houston, Texas plant. These grades are processed for use in plastics, rubber, coatings,.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 100% passing |
CIMBAR BariScan Elite Chemically Purified White Barium Sulfate (BaSO4) BariScan barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. BariScan and BariScan Ultra barite meet and exceed the requireme.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.0% retained |
CIMBAR CIMBAR™ CF Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.5% retained |
CIMBAR EliteTalc® 22 Cosmetic Talc Cimbar performance Minerals MV, LLC Talc U.S.P. Cosmetic talcs are designed specifically for cosmetic formulations. Talc is commonly used in cosmetics for its ability to bind to oils, create a mois.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.5% retained |
CIMBAR EliteTalc® 23 Cosmetic Talc Cimbar performance Minerals MV, LLC Talc U.S.P. Cosmetic talcs are designed specifically for cosmetic formulations. Talc is commonly used in cosmetics for its ability to bind to oils, create a mois.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 100% passing |
CIMBAR Miti-Wite B3 Chemically Purified White Barite (BaSO4) Miti-Wite barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. Miti-Wite products are available in a variety of particle sizes .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 55 - 65% passing, dry |
CIMBAR RMF 55 Recycled Mineral Filler Cimbar RMF is a locally sourced, third-party certified recycled filler containing 90% Post-Consumer materials. They are a clean, safe, environmentally-friendly alternative for use in various polyme.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 99.0% passing, wet |
CIMBAR Suspengel™ 325 Plus High Purity Bentonite, Industrial Grade Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process co.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 98% passing |
CIMBAR UltraMag & UltraMag ST 10 Magnesium Hydroxide Powder UltraMag is a naturally ground, white, high-purity Magnesium Hydroxide suitable for a wide range of applications including water treatment slurries, plastics, rubber and flame-retardant/smoke suppre.. |