Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 325 Mesh | 325 Mesh | 100% through |
Manufacturing Insight EFR-3 Enhanced Fire Retardant Additive EFR-3 is ideal for incorporation into unreinforced thermoset resin systems, including coatings and foams, potting compounds as well as electronic laminates and other similar applications. EFR-3 has .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.5% retained |
Imerys #6 Tileâ„¢ Kaolin #6 Tile is a high plasticity kaolin. It is well known for its contribution to high unfired strength plasticity and white fired properties. Information provided by Imerys. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 83% through; Alpine Air Jet Sieve |
Imerys 160D Ground Mica 160D is a dry Ground Mica (complex potassium aluminum silicate) with a controlled particle size distribution.Information provided by Imerys |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 78% through; Alpine Air Jet Sieve |
Imerys AMCâ„¢ Ground Mica AMC Mica is a dry Ground Mica (complex potassium aluminum silicate) with a controlled particle size distribution. The platy nature of AMC Mica contributes to improved crack resistance in formulted, .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 1% retained |
Imerys Barden™ AG-1 Kaolin Barden R is a Hydrated Aluminum Silicate available as an Air Float Beneficiated Fine Powder. This kaolin product is used as a high surface area “hard†filler for agricultural purposes.Info.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.5% retained |
Imerys Franklin™ R Kaolin Franklin R is an intermediate-grained Kaolin used as a filler is “soft†rubber products, plastic compounds, adhesives, protective coatings and similar applications.Information provided by .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | less than 0.01% retained |
Imerys Minsparâ„¢ 7 Ground Feldspar Minsparâ„¢ 7 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 7 is easily dispersed to a high Hegman grind to produce coatings with hig.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.005% Retained |
KaMin Hydrafine® 90W Clay Hydrafine® 90W is a premium quality, high brightness, fine particle size clay. Excellent for use in high brightness coated printing paper and board – providing a superb balance of print glo.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.005% Retained |
KaMin Hydrasperse® Kaolin Clay - Filler Hydrasperse® is a #2 coating clay available in standard and high brightness. Can be used over a wide range of coating applications.Industry: PAPER & PACKAGINGUses: Coated 1S Label, Coated Bleache.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.01% Retained |
KaMin KaMin® 100C Kaolin Clay - Calcined Calcined clay with new and unique processing and packaging, designed for applications requiring low moisture, such as 2 component urethanes. Prevents the need to pre-dry the mineral.Industry: Adhesi.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.005% Retained |
KaMin KaMin® HG Kaolin Clay - Waterwashed KaMin® HG is an economical, general purpose, water-washed kaolin with fine particle size and intermediate brightness. It is suitable for water borne paint, ink and adhesive applications.Industry:.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | Minimum of 70% |
H.C. Starck Amperweld® 1701.39 K4 Chromium Carbide RIII HS Number: 284990 |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 1% retained |
Silberline A-6205 A-6205 is a standard grade; class B, medium sized, leafing aluminum pigment carried in C-66 exempt mineral spirits.Applications: Trade & Maintenance |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.1% retained |
Silberline Extra Fine "O" Standard Series Extra Fine "O" - is a very fine, high opacity, non-leafing aluminum pigment for solvent based industrial coatings. Due to the small particle size, this grade is well suited for imparting high opacit.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.1% retained |
Silberline SilBerCote® PC 8153X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
Silberline Sparkle Silver® 5745 Sparkle Silver® 5745 is a fine, regular purity, non-leafing aluminum pigment with good opacity for solvent-based general industrial coatings. It provides excellent distinctiveness of image (D.O.I.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
Silberline Sparkle Silver® Premier 313AR Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
Silberline Tufflake® 5843 Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 2% retained |
Silberline Sparkle Silver® 3500 Sparkle Silver® 3500 is a medium, non-leafing aluminum pigment. It was developed to provide formulators of industrial finishes with an economical source of sparkling aluminum flake. It is widely .. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
Silberline Sparkle Silver® Premier 454 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
Silberline Sparkle Silver® Premier 552 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.1% retained |
Silberline Super Fine "N" Standard Series Super Fine N - is an ultra fine, high opacity, non-leafing aluminum pigment for solvent based industrial coatings. Due to the small particle size, this grade is well suited for imparting high opacit.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.1% retained |
Silberline Tufflake® 2222-AR Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 100% passes |
Excalibar ExBar™ W 3 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 98.0% passes |
Excalibar ExBar™ W 325 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | <0.2 g/l residues |
Dow Latex XZ 92226.00 Experimental Latex Description: XZ 92226.00 Experimental latex is an aqueous dispersion of a modified carboxylated styrene butadiene copolymer. It has been developed for use as latex for precoating and adhesive for se.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 99.5% passing |
CIMBAR Miti-Wite B10 Chemically Purified White Barite (BaSO4) Miti-Wite barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. Miti-Wite products are available in a variety of particle sizes .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.5% retained |
CIMBAR RiverCal™ 8107 & 8107C Calcium Carbonate (CaCO3) RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.3% retained |
CIMBAR RiverCal™ 8105 & 8105C Calcium Carbonate (CaCO3) RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.95 |
ATI Wah Chang Reactor Grade Zirconium Oxide, ZrO2 Reactor Grade. A white, free-flowing powder.Information provided by ATI Wah ChangTypical Analysis: On Zr metal basis |