Manufacturing Insight EFR-3 Enhanced Fire Retardant Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Manufacturing Insight LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Manufacturing Insight EFR-3 Enhanced Fire Retardant Additive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EFR-3 is ideal for incorporation into unreinforced thermoset resin systems, including coatings and foams, potting compounds as well as electronic laminates and other similar applications. EFR-3 has been proven especially successful in phenolic matrices, but also functions well in epoxy and urethane resin systems.When blended into a resin system, EFR-3 will react to heat and/or flame by foaming and forming a thick, high yield char barrier. The char barrier will extinguish fire and prevent further flame spread. Additionally, the char foam insulates and protects the polymer substrate from heat and fire damage.EFR-3 is halogen-free, contains no metals, PBDEs, PBBs or other brominated compounds and does not evolve the highly toxic and corrosive gasses associated with many other fire retardant compounds. EFR-3 is a RoHS/WEEE compliant material. EFR-3 functions at loading levels in the range of 10%-20% by weight. Flame spread and smoke developed values (ASTM E-84) are typically 10/10 and under and are in compliance with UL 94V0, MSC.41 (64) and FAR 25.853.
Physical Properties Metric English Comments
Solubility in Water <= 1.0 %
<= 1.0 %
At 170°F
Particle Mesh Size 325 Mesh
325 Mesh
100% through
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Appearance Very fine free flowing white powder
Char Activation Temp 300°C
Char Forming Efficiency 99% Minimum
Purity 98% Minimum