Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 200 - 700 cP | 200 - 700 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4151 SBR Latex ROVENE® 4151 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with above average strength properties. It may be compounded with a wide variety of fillers and additives.. |
|||
Brookfield Viscosity | 300 - 700 cP | 300 - 700 cP | Spindle # 3, rpm 60 |
Michelman® Coating X300™ Plus Water based, moisture and water resistant coating Description: Water based, moisture and water resistant coating.Usage: Coating X300™ Plus provides high levels of water resistance and good moisture resistance for kraft paper with improved wate.. |
|||
Brookfield Viscosity | 400 - 700 cP | 400 - 700 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Coat 82 Water resistance coating Description: Water resistance coating with intermediate moisture barrier and higher COF.Usage: Michem® Coat 82 is a repulpable, printable, and cold set gluable coating optimized for water resista.. |
|||
Brookfield Viscosity | 100 - 700 cP | 100 - 700 cP | Spindle # 3, rpm 60 |
Michelman® Micryl™ 766R Water resistant coating Description: General purpose water resistant coatingUsage: Micryl™ 766R is a water and grease resistant coating that can also function as a heat resistant gloss overprint. In such applications,.. |
|||
Brookfield Viscosity | 100 - 700 cP | 100 - 700 cP | Spindle # 3, rpm 60 |
Michelman® SofTak® 126 Non-skid coating Description: Non-skid coating.Usage: SofTak® 126 is a gluable nonskid coating with the added benefit of good scuff and water resistance, oil resistance and a "leather like" feel. This product is .. |
|||
Brookfield Viscosity | 500 - 700 cP @Temperature 25.0 °C |
500 - 700 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 501 Neopentylic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 501: Resin for high-.. |
|||
Brookfield Viscosity | 500 - 700 cP @Temperature 25.0 °C |
500 - 700 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 801 Neopentylic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 801: Resin for gel-c.. |
|||
Brookfield Viscosity | 450 - 700 cP | 450 - 700 cP | RVF #2 sp @ 20 rpm @ 80°F |
3M Scotch-Weld™ 10 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 10 is a multi-purpose contact adhesive which may be used to bond plastic laminate, aluminum, steel, wallboard, wood, masonry, rubber and canvas.Informati.. |
|||
Brookfield Viscosity | 500 - 700 cP | 500 - 700 cP | LVF sp #2 @30 rpm |
3M Scotch-Weld™ EC600 General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |