Material Notes:
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 501: Resin for high-quality gel-coatsInformation provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Brookfield Viscosity 500 - 700 cP

@Temperature 25.0 °C
500 - 700 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 - 90.0 °C
190 - 194 °F
Chemical Properties Metric English Comments
Styrene Content 37 - 39 %
37 - 39 %