Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 405 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 405 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Goo.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 406 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 406 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Goo.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 440 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 440 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Eur.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 455 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 455 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Goo.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 5585 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 5585 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Eu.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® CC 136 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® CC 136 is an aqueous dispersion of a modified carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers.Key Features: Europrene Latice® CC 136 shows .. |
|||
Brookfield Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya COVERCARB® 85 Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating that is designed to provide maximum opacity and maximum gloss. It is an excellent choice to reduce the demand for expensive pigments.. |
|||
Brookfield Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya OMYAPAQUE® Calcium Carbonate An ultrafine ground calcium carbonate for paper and board filling. An opacifying product that is designed to reduce costs through the replacement of more expensive pigments.Information supplied by O.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Hour Viscosity @ 6rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 171 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Hour Viscosity @ 6rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 4195 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Hour Viscosity @ 6 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L100UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L100UF is a medium molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for th.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Day Viscosity @ 30 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L100UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L100UF is a medium molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for th.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Hour Viscosity @ 6 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L120UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L120UF is a high molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for thin.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 5583 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 5583 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Go.. |
|||
Brookfield Viscosity | <= 300 cP | <= 300 cP | #20/200 |
Mallard Creek Polymers Rovene® 6018 Styrene-Acrylic Emulsion Applications: Rovene® 6018 is a silanated styrene-acrylic emulsion specifically designed for formulation of construction adhesives such as ceramic tile mastics and carpet adhesives. It provides e.. |
|||
Brookfield Viscosity | <= 300 cP | <= 300 cP | #20/200 |
Mallard Creek Polymers Rovene® 6118 Styrene-Acrylic Emulsion Applications: Rovene® 6118 is a silanated styrene-acrylic emulsion specifically designed for formulation of concrete sealers and performance coatings. It provides excellent adhesion to concrete a.. |
|||
Brookfield Viscosity | 300 - 750 cP | 300 - 750 cP | Spindle # 3, rpm 20 |
Michelman® Michem® Coat 95 Water and grease resistant, heat sealable coating Description: Water and grease resistant, heat sealable coatingUsage: Michem® Coat 95 is a good multi-purpose coating that provides excellent water, oil and grease resistance. This product is heat.. |
|||
Brookfield Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
ASTM D2196-86; LVT |
Lord Adhesives Aeroglaze® Z307 Absorptive Conductive Polyurethane Aeroglaze® Z307 black absorptive conductive polyurethane coating is primarily for application to substrates used on spacecraft. These applications include those where coatings must exhibit low ou.. |
|||
Brookfield Viscosity | <= 300 cP | <= 300 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 91240G Nonionic polyethylene emulsion Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 91240G is an additive which provides excellent anti-blocking, slip properties and mar resistance. It is also used as an additive.. |
|||
Brookfield Viscosity | 300 - 800 cP | 300 - 800 cP | Spindle # 3, rpm 60 |
Michelman® Release Coat® P1 Uncatalyzed portion of a two-part silicone release coating Description: Uncatalyzed portion of a two-part silicone release coatingUsage: Release Coat® P1 is one part of a two part silicone release coating. A catalyzed release coat system offers superior .. |
|||
Brookfield Viscosity | <= 300 cP | <= 300 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Tite 242AF Skin packaging primer Description: Skin packaging primerUsage: Michem® Tite 242AF is a coating designed to provide a tenacious bond between corrugated and either Surlyn or polyethylene clear skin pack films, firmly tr.. |
|||
Brookfield Viscosity | 300 - 1000 cP | 300 - 1000 cP | 1% at pH5, RVT N°2 at 20 rpm; AN2131 |
Solvay JAGUAR® EXCEL Surfactant Description: Clear grade with excellent wet combing and detangling benefits. Recommended for use in a broad range of conditioning shampoos.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: G.. |
|||
Brookfield Viscosity | 300 - 1000 cP | 300 - 1000 cP | RVT 20 rpm, spindle 2, after equilibration at 25°C for 1 h; AN2118 |
Solvay JAGUAR® C 162 Surfactant Description: Clear grade with light hair feel. Enhanced deposition of dimethicone oil on damaged hair.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: HYDROXYPROPYL GUAR HYDROXYPROPYLTRIMON.. |
|||
Brookfield Viscosity | 300 cP @Temperature 190 °C |
300 cP @Temperature 374 °F |
|
Westlake Epolene® E-25 Chemically Modified Polypropylene, Maleation Processed Product Description: Epolene E-25 is a maleic anhydride grafted polypropylene recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emul.. |
|||
Brookfield Viscosity | 300 cP @Temperature 190 °C |
300 cP @Temperature 374 °F |
|
Westlake Epolene® E-43 Chemically Modified Polypropylene, Maleation Processed Product Description: Epolene E-43 is a maleic anhydride grafted polypropylene recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emul.. |
|||
Brookfield Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
|
Loctite® 3105 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
|
Loctite® 363 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | <= 300 cP | <= 300 cP | #2 @ 50 rpm |
Dow Latex XZ 92229.00 Experimental Latex Description: XZ 92229.00 Experimental latex is an aqueous dispersion of a modified carboxylated styrene butadiene copolymer. It has been developed for use as a secondary backing latex for tufted car.. |
|||
Brookfield Viscosity | 300 - 400 cP @Temperature 25.0 °C |
300 - 400 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 103 L Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 103 L: Light-stabili.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | Mixed |
BCC Products DP-11-90 Urethane Casting DP-11-90 is an unfilled, low viscosity, quick setting two component urethane system. An easy to use 1 to 1 mix ratio (Part A/Part B), DP-11-90 offers the user a 3 minute working time with parts demo.. |