PolyOne Geon™ 170 Series L100UF Polyvinyl Chloride Homopolymer (PVC Homopolymer)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ 170 Series L100UF Polyvinyl Chloride Homopolymer (PVC Homopolymer).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Geon® Ultrafine 170-L100UF is a medium molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for thin film applications, and ability to produce even thinner gauge coatings. The excellent dispersibility provides good product throughput during the organosol manufacturing process with the sand milling process reduction or elimination. A medium molecular weight resin provides a good balance of fused film properties and processing temperatures. The low residual emulsifier level provides good end product performance in the areas of clarity, moisture blush resistance, low taste and odor. This resin is accepted by FDA for use under 21CFR175.300 (food contact application).Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® STP 1434 (formulation): 100phr Geon® L100UF, 55phr Aromatic100, 20phr Drapex 334-F, 5phr ESO, and 3phr Therm-Chek SP 120 LOHFInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Bulk Density 0.272 g/cc
0.00983 lb/in³
Fineness 6.0
6.0
Hegman, North Fineness; Geon® STP 1434
Relative Viscosity 2.37 cP
2.37 cP
Correlation, Cyclohexanone 1%; Internal Method
Brookfield Viscosity 200 cP
200 cP
One Hour Viscosity @ 30 rpmGeon® STP 1434 (with provided formulation); Internal Method
300 cP
300 cP
One Hour Viscosity @ 6 rpmGeon® STP 1434 (with provided formulation); Internal Method
300 cP
300 cP
One Day Viscosity @ 30 rpmGeon® STP 1434 (with provided formulation); Internal Method
525 cP
525 cP
One Day Viscosity @ 6 rpmGeon® STP 1434 (with provided formulation); Internal Method
Viscosity Measurement 1.0
1.0
Inherent; ASTM D1243-60-A
Processing Properties Metric English Comments
Moisture Content 0.070 %
0.070 %
Karl FisherGeon® STP 683; Internal Method
Descriptive Properties Value Comments
Clean Point 5.5 Hegman
Internal Method; GrindGeon® STP 1434 (with provided formulation)
Features High Clarity
Low to No Odor
Low to No Taste
Forms Powder
Fine, White Powder
Generic Material PVC Homopolymer
Generic Name Polyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value 70
No Standard; Correlation, 0.5g/100ml
Methanol Extractables 1.3%
Internal Method; Geon® STP 894
Polymerization Process Emulsion
Processing Method Casting
Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Residual Vinyl Chloride Monomer < 1 ppm
Internal Method; Geon® STP 1005
Uses Coating Applications
Film
Protective Coatings