Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 200 cP | 200 cP | dry |
Omya OMYACARB® F - FL Calcium Carbonate A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water.. |
|||
Brookfield Viscosity | 200 cP @Temperature 25.0 °C |
200 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya OMYAFIL® 60 Calcium Carbonate A fine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Brookfield Viscosity | 200 cP @Temperature 25.0 °C |
200 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya OMYAFIL® Calcium Carbonate An ultrafine ground calcium carbonate for paper and board filling.Information supplied by Omya North America. |
|||
Brookfield Viscosity | 200 cP @Temperature 25.0 °C |
200 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya OMYAFLOW® F - SY Calcium Carbonate A high purity, fine, wet ground natural calcium carbonate available in slurry form.Applications: Decorative paints.Information supplied by Omya North America. |
|||
Brookfield Viscosity | 200 cP @Temperature 25.0 °C |
200 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya OMYAFLOW® UF - SY Calcium Carbonate A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Decorative paints.Information supplied by Omya North America. |
|||
Brookfield Viscosity | 200 cP | 200 cP | One Day Viscosity @ 30rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 4195 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Brookfield Viscosity | 200 cP | 200 cP | One Hour Viscosity @ 30 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L100UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L100UF is a medium molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for th.. |
|||
Brookfield Viscosity | 200 cP | 200 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 1251 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 1251 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains an antioxidant.Key Features: Europrene Lati.. |
|||
Brookfield Viscosity | 200 - 400 cP @Temperature 20.0 °C |
200 - 400 cP @Temperature 68.0 °F |
Brookfield RVF sp. 2, 20 rpm solution at 15% in MEK; MQSA N0 40A |
Lubrizol Advanced Materials Pearlstick® 45-50/03 Linear Thermoplastic Polyurethane Elastomer
(discontinued ** Pearlstick 45-50/03 is an elastic, linear, aromatic polyurethane with an extremely high crystallization rate and a medium-low thermoplasticity level, available as pellets.Solubility: Pearlstick 45-.. |
|||
Brookfield Viscosity | 200 - 800 cP | 200 - 800 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4220 SBR Emulsion ROVENE® 4220 is a new developmental polymer specifically designed to be used flooring adhesives as well as an extender for chloroprene and natural latex in contact adhesives and other cohesive an.. |
|||
Brookfield Viscosity | 200 - 1500 cP | 200 - 1500 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4487 SBR Latex ROVENE® 4487 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is cross-linkable with external .. |
|||
Brookfield Viscosity | 200 - 1000 cP | 200 - 1000 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 5550 SBR Latex ROVENE® 5550 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with outstanding strength properties. This Self-crosslinking binder imparts excellent water and solvent r.. |
|||
Brookfield Viscosity | <= 200 cP | <= 200 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 6014 Acrylic Emulsion Applications: Rovene® 6014 is a self crosslinking acrylic polymer providing a stiff hand to frothed or saturated substrates. Rovene® 6014 is recommended for various nonwoven and paper applicat.. |
|||
Brookfield Viscosity | 200 - 600 cP | 200 - 600 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 6130 SBR Latex ROVENE® 6130 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of masking and carton sealing tape adhesives. It exhibits excellent compati.. |
|||
Brookfield Viscosity | <= 200 cP | <= 200 cP | Spindle # 2, rpm 60 |
Michelman® DigiGuard® Gloss 110 Overprint varnish Description: Overprint varnish for flexible packagingUsage: DigiGuard® Gloss 110 is a high gloss, temperature resistant, water based overprint varnish which meets FDA food contact requirements.Ap.. |
|||
Brookfield Viscosity | 200 - 1000 cP | 200 - 1000 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Dispersion 91530 Acrylic resin dispersion Michem® Dispersion 91530 is an additive used as a leveling aid, gloss enhancer and for buffability and mar resistance for the floor finish industry. This product is also effective for gloss enhan.. |
|||
Brookfield Viscosity | <= 200 cP | <= 200 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 21930 Anionic Tung Oil emulsion Description: Anionic Tung Oil emulsionUsage: Michem® Emulsion 21930 is a Tung Oil emulsion that contains 99.5% natural ingredients. It is used an additive that imparts good water bead to wood an.. |
|||
Brookfield Viscosity | <= 200 cP | <= 200 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 48040M2 Nonionic microcrystalline wax emulsion Description: Nonionic microcrystalline wax emulsionUsage: Michem® Emulsion 47950 is a wax emulsion which is effective as an anti-graffiti and sacrificial coating and can also contribute water res.. |
|||
Brookfield Viscosity | 200 - 850 cP | 200 - 850 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Prime 4990R Ethylene acrylic acid dispersion Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 4990R provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent r.. |
|||
Brookfield Viscosity | 200 - 625 cP | 200 - 625 cP | Spindle # 3, rpm 60 |
Michelman® Release Coat® 40 Water based release coating Description: One component, water based release coatingUsage: Release Coat® 40 is an easy-to-use one component silicone emulsion coating that provides superior release for a variety of "sticky" p.. |
|||
Brookfield Viscosity | 200 - 1800 cP | 200 - 1800 cP | 1% sol. in 1% KCl Brookfield LV 60 rpm spindle n°3; TI-1110 |
Solvay RHODOPOL® 23 Surfactant Description: Rhodopol® 23 is Standard grade Xanthan Gum. It exhibits high pseudoplastic behavior and rapid hydration rate. This grade is registered on the FALCON list of approved substances.Ident.. |
|||
Brookfield Viscosity | 200 cP | 200 cP | RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in MEK |
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane Features: High tensile strength, low temperature flexibility, and high adhesion to various substrates such as PET, PVC, and various fabrics.Uses: Fabric coating and audio tape binder, inks and solut.. |
|||
Brookfield Viscosity | 200 - 600 cP @Temperature 20.0 °C |
200 - 600 cP @Temperature 68.0 °F |
Brookfield RVT spindle 2.2 RPM |
C.O.I.M. FILCO® 352 Unsaturated Bisphenolic Polyester Polymer for Glass Fiber Sizing Description: Unsaturated Bisphenolic Polyester Polymer for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in .. |
|||
Brookfield Viscosity | 200 - 325 cP | 200 - 325 cP | RVF #2 sp @ 20 rpm |
3M Scotch-Weld™ 1099-L Nitrile High Performance Plastic Adhesives Features: It is a low viscosity grade for spray application.Fast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions and sheeting. (Ma.. |
|||
Brookfield Viscosity | 200 - 450 cP | 200 - 450 cP | RVF #2 sp @ 20 rpm @ 80°F |
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |
|||
Brookfield Viscosity | 200 - 325 cP | 200 - 325 cP | RVF #2 sp @ 20 rpm @ 27°C |
3M Scotch-Weld™ 4491 Nitrile Industrial Adhesive Features: Low viscosity grade for spray applicationFast dryingProvides strong, flexible bondsResists weathering, water, fuels, oil and plasticizersBonds vinyl extrusions and sheeting (May stain ligh.. |
|||
Brookfield Viscosity | 200 - 400 cP | 200 - 400 cP | LVF Spindle #2 @ 30 rpm |
3M Scotch-Weld™ FLX300 Flexible Instant Adhesive 3M™ Scotch-Weld™ Flexible Instant Adhesive FLX (formerly PR851) is formulated for extended resistance to impact, vibration, stress, peel, and humidity applications. It is faster curing than 3M™ S.. |
|||
Brookfield Viscosity | 200 - 400 cP | 200 - 400 cP | LVF, sp 2 @ 30 rpm |
3M Scotch-Weld™ MG300 FLX Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Brookfield Viscosity | >= 200 cP | >= 200 cP | |
DuPont Performance Polymers AquaStik® AQS-2900 Polychloroprene Latex
(discontinued **) Aquastik™ polychloroprene latexes have been designed for the adhesives industry. They provide an environmentally friendly alternative to solvent-borne systems.This grade features fast break. 59% .. |
|||
Brookfield Viscosity | 200 - 650 cP @Temperature 23.0 °C |
200 - 650 cP @Temperature 73.4 °F |
|
Lucite International Series 500 Liquid Acrylic Resin LUCITE® LIQUID ACRYLIC RESINS SERIES 500For the manufacture of solid surface sheet & worktopsAmbient temperature curing resin with low VOC emissionsCan be used on batch or continuous in-line mixing.. |