Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 1000 cc/m²/day @Temperature 23.0 °C |
64.5 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Bicor™ 20MB666 OPP Film Product Description: Bicor 20MB666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines and is mainly propos.. |
|||
Oxygen Transmission Rate | 1000 cc/m²/day @Temperature 23.0 °C |
64.5 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Bicor™ 20MB668 OPP Film Product Description: Bicor 20MB668 is a high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provid.. |
|||
Oxygen Transmission Rate | 1000 cc/m²/day @Temperature 23.0 °C |
64.5 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 30MW648 OPP Film Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VTLS) coating. VLTS coating provides an excel.. |
|||
Oxygen Transmission Rate | 1000 cc/m²/day @Temperature 23.0 °C |
64.5 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Bicor™ 20MBT666 OPP Film Product Description: Bicor 20MBT666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. This film is specifically suitable for unprinted overwrapping, offering unique as.. |