Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 42 g/10 min @Load 10.0 kg, Temperature 220 °C |
42 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® MG94 ABS Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 200 °C |
42 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Melt Flow | 42 g/10 min @Load 1.20 kg, Temperature 300 °C |
42 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® OQ1060 PC Copolymer Optical quality, high flow, high purity Polycarbonate copolymer resin with reduced oxygen transmission for advanced DVD applications such as Limited Play DVD.This data was supplied by SABIC-IP for t.. |
|||
Melt Flow | 42 - 56 g/10 min @Load 21.6 kg, Temperature 190 °C |
42 - 56 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio > 70; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6753G (526H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 42 - 94.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
42 - 94.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Kazanorgsintez PE2NT 18-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 300 °C |
42 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 300 °C |
42 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 300 °C |
42 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific) Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade. |
|||
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 280 °C |
42 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr.. |
|||
Melt Flow | 42 g/10 min @Load 10.0 kg, Temperature 220 °C |
42 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO-1133 |
Chi Mei Polylac® PA-765B ABS - Flame Retardant F.R. Medium Impact |
|||
Melt Flow | 42 g/10 min @Load 3.80 kg, Temperature 200 °C |
42 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Melt Flow | 42 g/10 min @Load 3.80 kg, Temperature 200 °C |
42 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Melt Flow | 42 g/10 min @Load 3.80 kg, Temperature 200 °C |
42 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |