Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 15.0 - 300 microns | 0.591 - 11.8 mil | Average value: 52.7 microns Grade Count:109 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Thickness | 50.0 - 300 microns | 1.97 - 11.8 mil | |
LG Chemical LUTENE FB0300 LDPE Blown Film Grade Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the e.. |
|||
Thickness | 50.0 - 300 microns | 1.97 - 11.8 mil | |
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade Description: The physical and structural characteristics of LUTENE MB9500 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Powder coating, artific.. |
|||
Thickness | 30.0 - 300 microns | 1.18 - 11.8 mil | possible range, depending on extrusion conditions |
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: .. |
|||
Thickness | 45.0 - 300 microns | 1.77 - 11.8 mil | possible range, depending on extrusion conditions |
Total EVA 1005 VN 2 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 2 is made by a high pressure tubular process. Grade for transparent and resistant films. Contains an antioxidant.Application examples: Stretch, coextrusion, frozen food, agriculture fi.. |
|||
Thickness | 30.0 - 300 microns | 1.18 - 11.8 mil | possible range, depending on extrusion conditions |
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt.. |
|||
Thickness | 25.0 - 300 microns | 0.984 - 11.8 mil | possible range, depending on extrusion conditions |
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa.. |
|||
Thickness | 25.0 - 300 microns | 0.984 - 11.8 mil | possible range, depending on extrusion conditions |
Total EVA 1005 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 5 is made by a high pressure tubular process. Grade for films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Coextrusion, stretch .. |
|||
Thickness | 5.00 - 300 microns | 0.197 - 11.8 mil | Average value: 35.2 microns Grade Count:16 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Thickness | 12.7 - 300 microns | 0.500 - 11.8 mil | Average value: 49.9 microns Grade Count:219 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |