Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1570 - 3180 microns | 62.0 - 125 mil | Range of Thicknesses Available |
Rogers Corporation Poron® 4701-41-20 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
Thickness | 1570 - 4780 microns | 62.0 - 188 mil | Range of Thicknesses Available |
Rogers Corporation Poron® Shock Seal™ 4790-79-20 Urethane Foam, Industrial Grade Thickness: 0.062"- 0.188"Color: BlackInformation provided by Rogers Corporation. |
|||
Thickness | 1570 microns | 62.0 mil | Total |
3M 4116 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Thickness | 1570 microns | 62.0 mil | |
3M 4516 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Thickness | 1570 microns | 62.0 mil | Total |
3M 4516 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Thickness | 1570 microns | 62.0 mil | Total |
3M 4726 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Thickness | 1570 microns | 62.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 30300R062 0.062" (1.57 mm) Uncured Silicone Rubber on Kodacel Carrier Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberCarrier: KodacelAppearance: Red silicone gum on polymer linersThis data represents typical values for the production mate.. |
|||
Thickness | 1570 microns | 62.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 32140R062 0.062" (1.57 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma.. |
|||
Thickness | 1570 microns | 62.0 mil | Silicone; Arlon SQA-TMS-003 |
Arlon 41300R062 0.062" Uncured Silicone Rubber on Holland Cloth Design/Construction:Interleave: 3.0 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Holland ClothThis data represents typical values for the production material and should not be used as m.. |
|||
Thickness | 1570 microns | 62.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55591R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Product Use: Electrical insula.. |
|||
Thickness | 1570 microns | 62.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 55833R062 Mar Resistant Press Pad; 1.6 mm Cured Silicone Rubber with Fiberglass Substrate Mar Resistant Press Pad - Product is sold with two finishes options: 55833R062AC - "C-finish" and 55833R062DST - "Smooth with Talc"Design/Construction:Interleave: 3 mil PESide 1: Cured Silicone Ru.. |
|||
Thickness | 1570 microns | 62.0 mil | |
3M Bumpon™ SJ5216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 1570 microns | 62.0 mil | |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 1570 microns | 62.0 mil | |
3M Bumpon™ SJ6016 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 1570 microns | 62.0 mil | |
3M Bumpon™ SJ6216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 1570 microns | 62.0 mil | Tape |
3M Cushion-Mount™ 1060 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 1570 microns | 62.0 mil | Tape |
3M Cushion-Mount™ E1060 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 1570 microns | 62.0 mil | Tape |
3M Cushion-Mount™ E1060H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Thickness | 1570 microns | 62.0 mil | Tape |
3M Cushion-Mount™ E1860 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Thickness | 1570 microns | 62.0 mil | Tape |
3M Cushion-Mount™ E1860H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Thickness | 1570 microns | 62.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R37152W062 0.062" (1.57 mm) Cured Silicone Rubber Design/Construction:Side 1: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInform.. |
|||
Thickness | 1570 microns | 62.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R37642R062 0.062" (1.57 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Interleave: PolyethyleneSide 1: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, mater.. |
|||
Thickness | 1570 microns | 62.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon R37642R062 0.062" (1.57 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Interleave: PolyethyleneSide 1: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, mater.. |
|||
Thickness | 1570 microns | 62.0 mil | |
3M 4116 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Thickness | 1570 microns | 62.0 mil | overall; Arlon SQA-TMS-003 |
Arlon 55149R062 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass |
|||
Thickness | 1570 microns | 62.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 55359R062 62 mil Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materi.. |
|||
Thickness | 1570 microns | 62.0 mil | |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 1570 microns | 62.0 mil | Tape |
3M Cushion-Mount™ E1060 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Thickness | 1570 microns | 62.0 mil | |
3M 4726 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Thickness | 1570 microns | 62.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 32300R062 0.062" (1.57 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma.. |