Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Bumpon™ SJ5216 Resilient Rollstock

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Bumpon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Bumpon™ SJ5216 Resilient Rollstock.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Physical Properties Metric English Comments
Density 0.640 g/cc
0.0231 lb/in³
Thickness 1570 microns
62.0 mil
Mechanical Properties Metric English Comments
Hardness, Shore M 36
36
Polyurethane, soft foam
Peel Strength 9.12 kN/m
52.0 pli
90°, Adhesion to Polypropylene
9.64 kN/m
55.0 pli
90°, Adhesion to Polystyrene
9.64 kN/m
55.0 pli
90°, Adhesion to ABS
9.64 kN/m
55.0 pli
90°, Adhesion to Stainless Steel
9.64 kN/m
55.0 pli
90°, Adhesion to Aluminum
Compression Set 8.0 %
8.0 %
ASTM D1056
10 %
10 %
50% deflection; ASTM D1056
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 52.0 °C
126 °F
Application
66.0 °C
151 °F
Service
107 °C
225 °F
Intermittent Exposure
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Service
5.00 °C
41.0 °F
Application
Descriptive Properties Value Comments
Adhesive Type R-25 (synthetic rubber
Appearance Light Brown