Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 170 microns | 6.70 mil | |
Hexcel® HexForce™ GA045 Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |
|||
Thickness | 170 microns | 6.70 mil | ASTM D3652 |
3M 2515 Flat Back Paper Masking Tape 3M™ Flat Back Paper Masking Tape 2515 can be used for splicing, bundling, holding, fastening, tabbing and packaging applications.Information provided by 3M |
|||
Thickness | 170 microns | 6.70 mil | ASTM D3652 |
3M 256 Colored Paper Tape 3M™ Colored Paper Tape 256 can be used for masking, bundling, holding and splicing operations needing colors for identification.Information provided by 3M |
|||
Thickness | 170 microns | 6.70 mil | Total; ASTM D3652 |
3M 3320 HVAC Construction Aluminum foil/scrim/laminate. UL 723 Classified.Information provided by 3M |
|||
Thickness | 170 microns | 6.70 mil | Total; ASTM D3752 |
3M 5491 PTFE Extruded Film Tape 3M™ PTFE Extruded Film Tape has a film backing with a silicone adhesive.Information provided by 3M |
|||
Thickness | 170 microns | 6.70 mil | Prepreg thickness - glass style 2313 |
Arlon 25FR Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Thickness | 170 microns | 6.70 mil | Prepreg thickness - glass style 2313 |
Arlon 25N Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Thickness | 170 microns | 6.70 mil | ASTM D3652 |
3M 233+ High Performance Green Masking Tape 3M™ High Performance Green Masking Tape 401+/233+ is a green colored crepe paper masking tape for critical paint masking applications in the automotive, specialty vehicle, and industrial markets wh.. |
|||
Thickness | 170 microns | 6.70 mil | ASTM D3652 |
3M 401+ High Performance Green Masking Tape 3M™ High Performance Green Masking Tape 401+/233+ is a green colored crepe paper masking tape for critical paint masking applications in the automotive, specialty vehicle, and industrial markets wh.. |
|||
Thickness | 170 microns | 6.70 mil | Total without liner; ASTM D3752 |
3M 5421 Polyethylene Tape 3M™ Polyethylene Tape 5421 has a rubber adhesive which provides an excellent abrasion resistant surface.Information provided by 3M |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7920 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive .. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7924 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7931 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7983 Sheet Polyester Label Material Features:Matte coating is compatible with screen printing and resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. Variable information can be added by the end .. |
|||
Thickness | 170 microns | 6.70 mil | Total Thickness |
3M 9496LE High Strength Double Coated Tape with Adhesives 300LSE and 200MP 3M™ Double Coated Tape 9496LE with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7940 Aluminum Foil Label Material 3M™Aluminum Foil Label Materials are durable, thin gauge, 1145 H19 aluminum designed to meet a wide range of difficult nameplate application requirements. 3M™Aluminum Foil Label Materials 7800, 78.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7942 Aluminum Foil Label Material 3M™Aluminum Foil Label Materials are durable, thin gauge, 1145 H19 aluminum designed to meet a wide range of difficult nameplate application requirements. 3M™Aluminum Foil Label Materials 7800, 78.. |
|||
Thickness | 170 microns | 6.70 mil | Liner |
3M 7980 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |