Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1000 microns | 39.4 mil | |
Mapal Plastics Maplon Type H Polypropylene Sheet Properties : Good resistance to low temperatures, Moderate stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printing.Applications : Stationery, Printing.. |
|||
Thickness | 1000 microns | 39.4 mil | |
Mapal Plastics Maplon Type O Polypropylene Sheet Properties: Corona treated on both sides for offset and screen printing, Extended shelf life, Low stress whitening, Suitable for die cuttingApplications: Stationery products, Offset printed item |
|||
Thickness | 1000 microns | 39.4 mil | |
Mapal Plastics Maplon Type S Polypropylene Sheet Properties: Low stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printingApplications: Stationery, Packaging, House-hold productsand printed items |
|||
Thickness | 1000 microns | 39.4 mil | |
Mo-Sci Corporation GAI-40-I Green A Intruder Filter Glass Applications: Lead-free NVIS Green A Intruder filter glass for incandescent light sources.Information provided by Mo-Sci Corporation. |
|||
Thickness | 1000 microns | 39.4 mil | |
Mo-Sci Corporation GB-40-N Green B Filter Glass Applications: Lead-free NVIS Green B filter glass for white LED sources.Information provided by Mo-Sci Corporation. |
|||
Thickness | 1000 microns | 39.4 mil | |
Mo-Sci Corporation WB-40-N White B Filter Glass Applications: Lead-free NVIS White class B filter glass for white LED sources.Information provided by Mo-Sci Corporation. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9077-65 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9077-75 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9077-80 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9077-95 LMW Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9604-80C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9604-85 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9604-85C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9604-90C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9604-95 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9812A-90 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9812A-95 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
SMAC SMACWRAP® ST Damping Material, 0.10 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit.. |
|||
Thickness | 1000 microns | 39.4 mil | |
Zoltek Panex 30® Low Oxidation Knitted Carbon Fabric Low Oxidation Knitted Carbon FabricApplications include: Thermal Protection Systems, Heat Shields, Rocket Nozzles, Carbon-Carbon Brakes |
|||
Thickness | 1000 microns | 39.4 mil | laminate layer thickness |
Bond Laminates TEPEX® dynalite 408-C200(2)-FG290(2)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and f.. |
|||
Thickness | 1000 - 3000 microns | 39.4 - 118 mil | Average value: 1100 microns Grade Count:26 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9604-95 LMW Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9604-95C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Sylvin Technologies 9812A-80 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Thickness | 1000 microns | 39.4 mil | |
Mo-Sci Corporation B-40-N Blue Filter Glass Applications: Lead-free NVIS blue filter glass for Nichia White LED sources.Information provided by Mo-Sci Corporation. |
|||
Thickness | 1000 microns | 39.4 mil | |
Mo-Sci Corporation GA-40-I Green A Filter Glass Applications: Lead-free NVIS Green A filter glass for incandescent light sources.Information provided by Mo-Sci Corporation. |
|||
Thickness | 1000 microns | 39.4 mil | |
Mo-Sci Corporation YB-40-I Yellow B Filter Glass Applications: Lead-free NVIS Yellow class B filter glass for incandescent light sources.Information provided by Mo-Sci Corporation. |
|||
Thickness | 1000 microns | 39.4 mil | |
Mo-Sci Corporation YB-40-N Yellow B Filter Glass Applications: Lead-free NVIS Yellow class B filter glass for white LED sources.Information provided by Mo-Sci Corporation. |