Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 88.9 microns | 3.50 mil | |
Hexcel® HexForce™ 1608 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 88.9 microns | 3.50 mil | |
Hexcel® HexForce™ 220HT Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 88.9 microns | 3.50 mil | |
Hexcel® HexForce™ 120 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | >= 88.9 microns | >= 3.50 mil | Side 2 |
Arlon 28571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | >= 88.9 microns | >= 3.50 mil | Side 1 |
Arlon 51571XC015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51576XC015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Cured Silicone Rubber This data represents typical values for the production mat.. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51576XC15A 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the producti.. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51576XC15A 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the producti.. |
|||
Thickness | 88.9 microns | 3.50 mil | Total (excluding liner) |
3M 9740 Double Coated Tape 3M™ Double Coated Tape 9740 is a 3.5 mil double coated tape utilizing a 0.5 mil (12 microns) polyester film coated on both sides with 1.5 mils (38 microns) of a high shear acrylic adhesive system. .. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon Thermabond® 48991A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation IIa Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style .. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV052R Tire Vinyl Label Products 3M™ Tire Vinyl Label Products are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling tires when used w.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV055 Tire Vinyl Label Products 3M™ Tire Vinyl Label Products are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling tires when used w.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV062 Semi-Rigid White Vinyl Label Product 3M™ Semi-Rigid White Vinyl Label Products are white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clarity general.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV063 Semi-Rigid White Vinyl Label Product 3M™ Semi-Rigid White Vinyl Label Products are white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clarity general.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV091 Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV100K Soft White Vinyl EDP Label Product 3M™ Soft White Vinyl EDP Label Products FV100K and FV1002 are flexible vinyl label stocks that offer excellent durability and some moisture resistance. These vinyl labels utilize 3M™ Adhesive F220.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV232 Soft Yellow Vinyl Label Products 3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV233 Soft Yellow Vinyl Label Products 3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV392 Removable White Vinyl Label Products 3M™ Removable White Vinyl Label Products FV1172 and FV392 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive .. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV513 Semi-Rigid Vinyl Label Product 3M™ Semi-Rigid Vinyl Label Products are semi-rigid white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1410, which is a general purpose.. |
|||
Thickness | 88.9 microns | 3.50 mil | Prime Coated 2113 Fiberglass, Substrate |
Arlon 47576R007 0.0075" (0.190 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mate.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M 7122 Performance Paper Label Material 3M™ Label Materials 7120 and 7122 latex impregnated paper with 3M™ 400 and 320 adhesives offer good conformability to curved surfaces and resistance to staining and moisture. Label Material 7120 h.. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV026505 White Vinyl Label Products 3M™ White Vinyl Label Products are flexible and conformable materials that offer durability and moisture resistance. The polymerically plasticized nature of this soft vinyl imparts long term dimens.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV1002 Soft White Vinyl EDP Label Product 3M™ Soft White Vinyl EDP Label Products FV100K and FV1002 are flexible vinyl label stocks that offer excellent durability and some moisture resistance. These vinyl labels utilize 3M™ Adhesive F220.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV230 Soft Yellow Vinyl Label Products 3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar.. |
|||
Thickness | 88.9 microns | 3.50 mil | Release Liner |
3M 450XL Extended Liner Tapes 3M™ Extended Liner Tapes have a liner that extends beyond the width of the adhesive to provide easy liner starting and removal. The liners, with the exception of 3M™ Extended Liner Tape 450EK is p.. |
|||
Thickness | 88.9 microns | 3.50 mil | Adhesive |
3M 9653LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Thickness | 88.9 microns | 3.50 mil | Tape |
3M 9737R Double Coated Splicing Tape 3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres.. |
|||
Thickness | 88.9 microns | 3.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 47568R0055E 0.0075" (0.190 mm) Cured Silicone Rubber/Acrylic PSA Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 2113 FiberglassSide 2: Acrylic PSA Interleave: Polypropylene This data represents typical values for the production material. The.. |