Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 70.0 microns | 2.76 mil | |
P & P Technology Oriented Wires In Silicone P & P Technology SP, SS, SR, SW & SF Ranges of gasket materials consist of Monel or aluminum wires embedded into solid silicone, sponge silicone or fluorosilicone, a fire retardant variant is also a.. |
|||
Thickness | 70.0 - 127 microns | 2.76 - 5.00 mil | Average value: 82.4 microns Grade Count:7 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Thickness | 70.0 - 3180 microns | 2.76 - 125 mil | Average value: 821 microns Grade Count:17 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Thickness | 70.0 microns | 2.76 mil | |
Isoflon Tisoflon® 3G Polytetrafluoroethylene & Graphite Coated Glass Fabric PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon. |
|||
Thickness | 70.0 microns | 2.76 mil | |
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon. |
|||
Thickness | 70.0 microns | 2.76 mil | |
Borealis Borstar® FB4250T LLDPE for Blown Film Borstar FB4250 is well suited for a wide range of film applications due to its properties. The well balanced mechanical properties will improve the functionality of the films or allow for material .. |
|||
Thickness | 70.0 microns | 2.76 mil | Film |
Topas Advanced Polymers TOPAS® 5013F-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013F-04 is a high temperature film extrusion grade for blends. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity .. |
|||
Thickness | 70.0 microns | 2.76 mil | Film |
Topas Advanced Polymers TOPAS® 6013F-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013F-04 is a high temperature, general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and p.. |
|||
Thickness | 70.0 microns | 2.76 mil | Film |
Topas Advanced Polymers TOPAS® 8007F-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007F-04 is a general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and.. |
|||
Thickness | 70.0 microns | 2.76 mil | Film |
Topas Advanced Polymers TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC) TOPAS® 9506F-500 is a high clarity extrusion grade for use in shrink, food and medical packaging as either a discrete layer in multilayer film or in blends with polyethylene. It is designed to del.. |
|||
Thickness | 70.0 microns | 2.76 mil | Film |
Topas Advanced Polymers TOPAS® 8007F-400 Cyclic Olefin Copolymer (COC) TOPAS® 8007F-400 is a robust film extrusion grade designed for blending with polyethylene (PE). It is a moderate clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, .. |
|||
Thickness | 70.0 - 80.0 microns | 2.76 - 3.15 mil | |
CEN® Electronic Material CN Polyimide Film, 3 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Thickness | 70.0 - 80.0 microns | 2.76 - 3.15 mil | ASTM D374 |
CEN® Electronic Material CV Polyimide Film, 3 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |