Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 27.9 - 43.2 microns | 1.10 - 1.70 mil | Supported Adhesive |
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam Information provided by Rogers Corporation. |
|||
Thickness | 28.0 microns | 1.10 mil | ± 2.5%; ASTM-252-78 |
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 28 µm) PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c.. |
|||
Thickness | 28.0 microns | 1.10 mil | Using a 230 mesh stainless steel screen, 13 micron emulsion |
Gwent Electronic Materials C2040308D2 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 40/60. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste.. |
|||
Thickness | 27.9 microns | 1.10 mil | |
Hexcel® HexForce™ 104 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 27.9 microns | 1.10 mil | |
Chengdu Polyster 70 LPI Lenticular Lens Sheet, PP Specially designed for advertisement. It is used for posters, billboards, etc. The suitable graphic effects: flip, 3D, animation, morph, zoom, etc.Information provided by Chengdu Polyster Co., Ltd. |
|||
Thickness | 27.9 microns | 1.10 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 110 AXT OPP Film Product Description: Bicor ASB-X is a two side coated, sealable OPP film delivering an advanced level of moisture and oxygen battier protection. This film is designed for use in (unsupported and sur.. |
|||
Thickness | 27.9 microns | 1.10 mil | ExxonMobil Method |
ExxonMobil Bicor™ 29MB080 OPP Film Product Description: A biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a single web in HFFS.. |
|||
Thickness | 27.9 microns | 1.10 mil | |
ExxonMobil Hicor® 110 BIHD-ASB OHD Film One-side acrylic, one-side PVdC coated, oriented high density polyethylene film. This film provides tack seal capability and excellent deadfold. Information provided by ExxonMobil Chemical |
|||
Thickness | 27.9 microns | 1.10 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 28LLG MET OPP Film Product Description: A clear, one-side metallized, one-side treated oriented polypropylene film. The metalized layer is designed to provide a bright metal appearance in surface print or laminated ap.. |
|||
Thickness | 27.9 microns | 1.10 mil | ExxonMobil Method |
ExxonMobil Metallyte™ 28MWHB OPP Film Product Description: A multi-layer, cavitaed, white OPP film that has exceptional barrier to gases, flavors and moistures. It is metalized on one side with a proprietary sealant layer on the other. .. |
|||
Thickness | 27.9 microns | 1.10 mil | ExxonMobil Method |
ExxonMobil Metallyte™ 28UBW-ES OPP Film Product Description: A multi-layer, cavitaed, white OPP film with an enhanced sealant to allow sealing through contamination. This film has an exceptional barrier to gases, flavors, and moisture. It.. |
|||
Thickness | 27.9 microns | 1.10 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 110 ASB-X OPP Film Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. ASB-X is good for heavy .. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7026 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7042 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7046 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7046 and 7053 are durable, high performance materials that offer excellent durability and moisture resistance. These vinyl label stocks utilize.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7048 Screen Printable Extended Life Vinyl Performance Label Products 3M™ Screen Printable Extended Life Vinyl Performance Label Products are high performance materials that offer good conformability and moisture resistance. These vinyl label stocks utilize 3M™ Adhe.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M FP032305 White Metallized Polypropylene Label Products 3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesi.. |
|||
Thickness | 27.9 microns | 1.10 mil | Backing; ASTM D3652 |
3M Scotch® 3199 Security Message Box Sealing Tape Scotch® Security Message Box Sealing Tape 3199 is a performance packaging tape used specifically where the security of the carton contents is a concern. The printed design along with the message ma.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7031 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7033 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7035 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 27.9 microns | 1.10 mil | Facestock |
3M 7037 Screen Printable Polyester Performance Label Product 3M™ Screen Printable Polyester Performance Abel Product 7037 is a durable, high performance material that offers excellent thermal stability and moisture resistance. This polyester label stock util.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7053 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7046 and 7053 are durable, high performance materials that offer excellent durability and moisture resistance. These vinyl label stocks utilize.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7215SA Screen Printable Polyester Performance Label Products with Structured Adhesive 3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7218SA Screen Printable Polyester Performance Label Products with Structured Adhesive 3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc.. |
|||
Thickness | 27.9 microns | 1.10 mil | Backing; ASTM D3752 |
3M 853 Polyester Tape 3M™ Polyester Tape 853 is comprised of strong, thin polyester backing with high shear, solvent resistant acrylic adhesive. These qualities make this tape ideal for applications where solvent exposu.. |
|||
Thickness | 27.9 microns | 1.10 mil | Tape |
3M 9019 Double Coated Tapes with Adhesive 300 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides.. |
|||
Thickness | 27.9 microns | 1.10 mil | Backing; ASTM D3652 |
3M Scotch® 311 Box Sealing Tape Scotch® Box Sealing Tape 311 is a general purpose box sealing tape designed specifically for utility type applications on light to medium weight boxes. The product offers good performance over broa.. |
|||
Thickness | 27.9 - 12700 microns | 1.10 - 500 mil | Average value: 2230 microns Grade Count:26 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |