Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 760 microns | 29.9 mil | Standard |
GrafTech eGRAF® SPREADERSHIELD™ SS500 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Thickness | 760 microns | 29.9 mil | Standard; Laminate |
GrafTech GRAFOIL® GHN Standard Fluid Sealing Laminate, Non-Metal Reinforced GRAFOIL® Grade GHN is an unbranded laminate made with GRAFOIL® Grade TG-337 flexible graphite, thermally bonded to both faces of a plastic insert. It is not certified to any industry standards.. |
|||
Thickness | 760 microns | 29.9 mil | Standard |
GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTA premium flexible graphite is a non-inhibited grade developed for use in nuclear or semiconductor applications. It is certified to meet the most rigorous purity specifications of the .. |
|||
Thickness | 760 microns | 29.9 mil | Standard |
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall.. |
|||
Thickness | 760 microns | 29.9 mil | Standard |
GrafTech GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC c.. |
|||
Thickness | 760 microns | 29.9 mil | Standard |
GrafTech GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material GRAFOIL® GTJ premium flexible graphite is an oxidation/corrosion inhibited grade developed for use in nuclear and high temp, high purity applications. It is certified to meet the most rigorous pu.. |
|||
Thickness | 760 microns | 29.9 mil | Standard |
GrafTech GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material GRAFOIL® SUPER GTO® flexible graphite sheet is a gasketing material containing no binders, which will seal a wide variety of liquids and gases over an extremely large temperature range (-240Â.. |
|||
Thickness | 760 microns | 29.9 mil | Standard for Single-Sided Laminate |
GrafTech GRAFOIL® GRAFKOTE® Laminates, Non-Metal Reinforced GRAFOIL® GRAFKOTE® laminates are made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0005" thick polymer facing on one ("Single-Sided") or both ("Double-Sided") sides. Th.. |
|||
Thickness | 760 microns | 29.9 mil | Dry Thickness |
Zoltek Panex 35® Stitch-Bonded Uni-Directional Carbon Fiber Fabrics Stitch-Bonded Uni-Directional Carbon Fiber FabricsApplications include: Infrastructure, Body Panels, Wind Blade Spars |
|||
Thickness | 760 microns | 29.9 mil | |
3M Nextel™ BF-30 Woven Fabric 440 Information provided by 3M |
|||
Thickness | 760 microns | 29.9 mil | |
3M Nextel™ AF-30 Industrial Woven Fabric 312 Information provided by 3M |