Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 50.8 microns | 2.00 mil | |
LyondellBasell Purell® PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding Purell PE 1840 H is a low density polyethylene with good flexibility and is delivered in pellet form. It is designed for small blow molding but can also be used in film applications and injection mo.. |
|||
Thickness | 50.8 microns | 2.00 mil | 2:1 BUR; 25 mil die gap |
LyondellBasell Petrothene® NA362005 Low Density Polyethylene ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits.. |
|||
Thickness | 50.8 microns | 2.00 mil | 2:1 BUR; 25 mil die gap |
LyondellBasell Petrothene® NA480177 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Thickness | 50.8 microns | 2.00 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ ROSO 50LR210 OPP Film Product Description: A clear, machine-direction shrinkable, one-side treated, polypropylene film. This film is designed for use as a monoweb in roll-fed labeling of contoured containers, such as alu.. |
|||
Thickness | 50.8 microns | 2.00 mil | |
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene For high speed, thin film applications Additional thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Thickness | 50.8 microns | 2.00 mil | |
Dow DOWLEX™ 2070G Linear Low Density Polyethylene High strength in food packaging applications Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Thickness | 50.8 microns | 2.00 mil | |
Dow INTEGRAL™ 909 Monolayer Adhesive Film / Automotive Headliners INTEGRAL 909 Adhesive Film is a versatile heat-activated film that bonds to such substrates as: Polyethylene, Nylon, Polyester, Fiberglass, Polyurethane Foams, Wood, Paperboard, Cotton, Non-wovens,.. |
|||
Thickness | 50.8 microns | 2.00 mil | Backing |
3M 1120 EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Thickness | 50.8 microns | 2.00 mil | ASTM D3652 |
3M 2104 Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 2104 has a very low-tack adhesive system to helpInformation provided by 3M |
|||
Thickness | 50.8 microns | 2.00 mil | Backing; ASTM D3652 |
3M 4380 General Purpose Aluminum Foil Tape 3M™ Aluminum Foil Tape 4380 is a general purpose aluminum foil tape offering a dead soft aluminum foil backing combined with an acrylic pressure sensitive adhesive.Information provided by 3M |
|||
Thickness | 50.8 microns | 2.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 25662T010 0.010" (0.254 mm) Cured Silicone Rubber with Laminated ETFE Film Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: (ETFE offers good chemical resistance to the following classes of chemicals) Alkalis, Organic a.. |
|||
Thickness | 50.8 microns | 2.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 49442R0075EP 0.0075" (0.190 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Substrate: Style 1681 FiberglassSide 2: Acrylic PSAThis data Represents typical values for the production material. The data should not be used to w.. |
|||
Thickness | 50.8 microns | 2.00 mil | Adhesive |
3M 9673 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Controltac™ IJ3552C Changeable Graphic Film with Comply™ Adhesive 2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conformers to surface with corrugations and rivets; Air release channels for fast, easy, bu.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM06P Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FP08N Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ 3632-246 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ 3632-97 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ 8000LF-37 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Thickness | 50.8 microns | 2.00 mil | Side 1 |
Arlon 47576R007 0.0075" (0.190 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mate.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M 7911FL Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 50.8 microns | 2.00 mil | Side 2, Cured |
Arlon R33468A030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured LayersAppearance: Semi-cured blue silicone gum on glass fabricThis data Represents typical values for the production material. .. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Controltac™ 8620Cv3 ES Changeable Graphic Film with Comply™ v3 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM532 White Polyester Label Products 3M™ White Polyester Label Products FM53R2, FM532 and FM782 are durable, high performance materials that utilize 3M™ Adhesive P1110, which is for labeling tires when used with tire wash. This adhes.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 7725-53 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM04630K White Polyester Label Product 3M™ White Polyester Label Products FM046302 and FM04630K are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Ad.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ 3632-76 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 7725-57 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 50.8 microns | 2.00 mil | Side 1 |
Arlon 44426R010 0.010" Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Cured Silicone RubberSide 2: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassThis data represents typical values for the p.. |