Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.0 - 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 - 13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 11 - 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 - 13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polyplastic Armlen® PP MF 30-3IM Polypropylene, 30% Mineral Filled UV resistant, impact modified, heat stabilizedInformation provided by PolyPlastic Group. |
|||
Melt Flow | 10 - 13 g/10 min @Load 2.16 kg, Temperature 380 °C |
10 - 13 g/10 min @Load 4.76 lb, Temperature 716 °F |
6`; ASTM D1238 |
Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Melt Flow | 8.0 - 13 g/10 min | 8.0 - 13 g/10 min | ASTM D1238 |
Kolon KOCETAL® K300LO Low Odor Acetal Resin Low odor of formaldehyde gas. Applications: Products for low odor. Information provided by API-Kolon. |
|||
Melt Flow | 10 - 13 g/10 min | 10 - 13 g/10 min | ASTM D1238 |
Kolon KOCETAL® UR302 Toughened Grade Acetal Resin TPU added, improved toughness. Applications: Impact resistant, flexible products. Information provided by API-Kolon |
|||
Melt Flow | 10.5 - 13 g/10 min | 10.5 - 13 g/10 min | ASTM D1238 |
Kolon KOCETAL® VT301 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |
|||
Melt Flow | 10 - 13 g/10 min | 10 - 13 g/10 min | ASTM D1238 |
Kolon KOCETAL® WR301 Wear Modified Acetal Resin Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Melt Flow | 10 - 13 g/10 min | 10 - 13 g/10 min | ASTM D1238 |
Kolon KOCETAL® WR301LO Wear Modified Acetal Resin Improved weather resistance and low odor of FA. Applications: Weather resistant products at closed space. Information provided by API-Kolon. |
|||
Melt Flow | 10 - 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 - 13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PC-1000RX Biocompatible Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications.All information provided by LTL Color Compounders, Inc. |
|||
Melt Flow | 10 - 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 - 13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PC-1001A Antimicrobial Polycarbonate A 10 melt grade of Polycarbonate containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders.. |
|||
Melt Flow | 10 - 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 - 13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PC-1002AF Food Grade Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Melt Flow | 10 - 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 - 13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PC-1002ARX Biocompatible Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Melt Flow | 10 - 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 - 13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PC-1005ARX Biocompatible Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Col.. |
|||
Melt Flow | 5.0 - 13 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.0 - 13 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Kraton® D1160 B (SIS) Linear Triblock Copolymer Description: Kraton D1160 B is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from South America in the physical form identified: Kr.. |
|||
Melt Flow | 7.0 - 13 g/10 min @Load 5.00 kg, Temperature 200 °C |
7.0 - 13 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kraton® D1114 P (SIS) Linear Triblock Copolymer Description: Kraton D1114 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 19%. It is supplied from North America in the physical form identified: .. |
|||
Melt Flow | 8.0 - 13 g/10 min | 8.0 - 13 g/10 min | ISO 1133 |
Chengdu Polyster H5550 Thermoplastic Polyether-ester Elastomer (TPEE) Medium-low modulus molding and injection grade. Contains improved color- stable antioxidants. Good balance of low and high temperature properties. Applications requiring high original color retentio.. |
|||
Melt Flow | 8.0 - 13 g/10 min | 8.0 - 13 g/10 min | ISO 1133 |
Chengdu Polyster H6555 Thermoplastic Polyether-ester Elastomer (TPEE) Medium modulus molding and extrusion grade. Contains improved color- stable antioxidants. Good balance of modulus and toughness. Parts and components of automobile, hydraulic hose and slide of eleva.. |
|||
Melt Flow | 9.0 - 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 - 13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Cossa Polimeri ESTALENE EN 10 C Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 9.0 - 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 - 13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Cossa Polimeri ESTALENE EN 10 SC Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 9.0 - 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 - 13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Cossa Polimeri ESTALENE EN 10 SSC Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 9.0 - 13 g/10 min @Load 0.325 kg, Temperature 190 °C |
9.0 - 13 g/10 min @Load 0.716 lb, Temperature 374 °F |
die 8/2; ISO 1133 |
Addcomp PRIEX® 20093 Maleic Anhydride Grafted PP homopolymer Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fiber, wood flour, natural fibers, multilayer films, aluminum foils, or mineral filled polypr.. |
|||
Melt Flow | 10 - 13 g/10 min | 10 - 13 g/10 min | |
Ashley Polymers Ashlene® 1641 Polycarbonate A general purpose injection molding grade, natural resin, UL approved. Also available as: 1641R (with release); 1643 (with UV stabilizers); 1643R (with release and UV stabilizers).Data provided by .. |
|||
Melt Flow | 9.0 - 13 g/10 min | 9.0 - 13 g/10 min | |
Biomer P226 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |
|||
Melt Flow | 10 - 13 g/10 min | 10 - 13 g/10 min | |
Ashley Polymers Ashlene® 1041BU Polycarbonate A general purpose injection molding grade, in black. Also available as: 1043BU (with UV stabilizers).Data provided by the manufacturer |
|||
Melt Flow | 11 - 13 g/10 min @Load 5.00 kg, Temperature 200 °C |
11 - 13 g/10 min @Load 11.0 lb, Temperature 392 °F |
Granulate; ISO 1133/H |
SYNTHOS Krasten® 336M High Impact Polystyrene Easy flow grade. Processed by injection moulding of intricate and thin-walled products that enables high production output.Synthos was formerly known as Kaucuk. All information provided by Synthos. |