Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.61 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 5.75 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC BF315 LDPE Characteristics: Good Processability and Excellent Optical PropertiesApplications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.61 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 5.75 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties. Good Optical Properties. Additives : No Additive Applications: Agricultural FilmCSA No. 25895-47-0Information provided by LG Chemical |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.61 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 5.75 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCSA No. 24937-78-8Information provided by LG Chemical |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC ST308 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC ST318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Melt Flow | 0.40 - 1.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.40 - 1.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 9401 Injection Molding Grade, Ultra High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 0.40 - 1.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.40 - 1.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 9501 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC SF316 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Additives- Medium slip agent, Medium antiblocking agentApplications: Agricultural & i.. |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC SF318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati.. |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC SN318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati.. |