Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman M3006-P Polyethylene
(discontinued **) Medium density polyethylene M3006-P is a specialty formulation suggested for high speed extrusion coating applications. M3006-P offers improvements over low density polyethylene in barrier properti.. |
|||
Melt Flow | 4.4 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.4 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Melt Flow | 4.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM-D1238 |
Ineos ABS Lustran® 451 ABS, Injection Molding Grade Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss. |
|||
Melt Flow | 4.4 g/10 min | 4.4 g/10 min | ISO 1133 |
Lucite International Diakon® CMG302 Acrylic Polymer Information provided by Lucite International |
|||
Melt Flow | 4.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Techmer ES HiFill® HDPE 8904 UV GY Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Melt Flow | 4.4 g/10 min @Load 2.20 kg |
4.4 g/10 min @Load 4.86 lb |
ASTM D1238 |
Sumitomo Chemical ESPOLEX® WT487X Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Melt Flow | 4.4 g/10 min @Load 5.00 kg, Temperature 230 °C |
4.4 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Chi Mei Polylac® PA-747S ABS - Extrusion High Impact Extrusion |
|||
Melt Flow | 4.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA M-143 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 4.4 g/10 min | 4.4 g/10 min | ASTM D1238 |
Huntsman Rexell® L3103 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent optics and sealability with good toughnessApplications: Stretch wrap and coextruded film for general packaging.FD.. |
|||
Melt Flow | 4.4 g/10 min | 4.4 g/10 min | ASTM D1238 |
Huntsman Rexell® M3107 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, .. |
|||
Melt Flow | 4.4 g/10 min | 4.4 g/10 min | ASTM D1238 |
Huntsman Rexell® V3101 Blown Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, cast film extrusion, FDA compliant.Features: High toughness, puncture resistance with good sealing and excellent optical properties.Applications: Food packagin.. |
|||
Melt Flow | 4.4 g/10 min | 4.4 g/10 min | ISO 1133 |
Lucite International Diakon® MG102 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |