Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 190 °C |
27 g/10 min @Load 22.0 lb, Temperature 374 °F |
ISO 1133 |
Multibase TPSiV® 4200-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers Kepital® F30-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 27 g/10 min @Load 1.20 kg, Temperature 300 °C |
27 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 905AU PC (Asia Pacific) LEXAN resin grade 905AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in all colors, intended to .. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 400 °C |
27 g/10 min @Load 11.0 lb, Temperature 752 °F |
ASTM D1238 |
Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2401 is a high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature o.. |
|||
Melt Flow | 27 - 37 g/10 min @Load 10.0 kg, Temperature 420 °C |
27 - 37 g/10 min @Load 22.0 lb, Temperature 788 °F |
ASTM D1238 |
Mitsui AURUM® JCL3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Melt Flow | 27 - 37 g/10 min @Load 10.0 kg, Temperature 420 °C |
27 - 37 g/10 min @Load 22.0 lb, Temperature 788 °F |
ASTM D1238 |
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCN3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 230 °C |
27 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Pro-fax PF531 Polypropylene Homopolymer, Radiation Resistant Primary Processing Method: Injection MoldingKey Features: high melt flow, radiation-resistant polypropylene homopolymer resin, excellent retention of physical properties and color after radiation st.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical Lucet® N127 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | ASTM D1238 |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | ASTM D1238 |
Kolon KOCETAL® K700BK Colored Grade Acetal Resin Colored, low viscosity grade.Applications: Thin products, improved appearance.Information provided by API-Kolon. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 220 °C |
27 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 275 °C |
27 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO/FDIS 1133 |
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 260 °C |
27 g/10 min @Load 4.76 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Valox® VX7024 PBT (Europe-Africa-Middle East) VALOX VX7024 is a 12% mineral filled PBT injection moulding resin with excellent mechanical properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 300 °C |
27 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL ZM3242 PPE+PS (Asia Pacific) Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degC |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 230 °C |
27 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SCG Chemicals EL-Proâ„¢ P740J Polypropylene Injection Molding Key Characteristics:Good flowabilityGood processabilityHigh stiffnessRecommended Applications:Automotive, motorcycle and electrical appliance parts that require good flowability such as automotive t.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 230 °C |
27 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis HG455FB Polypropylene Homopolymer HG455FB is a polypropylene homopolymer intended for fiber applications. Applications: fine filament count at high spinning speeds, spun bonded nonwovens, and POY production.Information provided by .. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Wico Plast Wicotal 270 Acetal ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 240 °C |
27 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
Cossa Polimeri ESTABLEND PA 3000 ABS / Nylon 6 Blend ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri.. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 265 °C |
27 g/10 min @Load 11.0 lb, Temperature 509 °F |
cm³/10 min. |
Covestro Makroblend® UT-250 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 500 LS POM High flow injection molding grade based on Tarnoform 500 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Barlog Plastics KEBAFORM C 274 VT POM Copolymer unreinforced, antistatic POMInformation provided by BARLOG plastics GmbH. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 250 °C |
27 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
BASF Ultradur B 4300 G6 LS High Speed BK15045 30% Glass Filled PBT |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | |
Ashley Polymers Ashlene® 195-N2 Acetal A general purpose, medium viscosity natural.Data provided by the manufacturer |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | |
Ashley Polymers Ashlene® 197-N2 Acetal A general purpose, very low viscosity, in natural.Data provided by the manufacturer |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BLUESTAR BS270 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
PTS POM-270 Acetal Copolymer Information provided by PTS LLC. |