Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 26 g/10 min @Load 3.80 kg, Temperature 230 °C |
26 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 41 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 26 g/10 min | 26 g/10 min | ASTM D1238 |
Mytex Polymers AS88L-01 Polypropylene, Compounded, Elastomer Description: AS88L-01 is a compounded, elastomer modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications .. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 190 °C |
26 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Flexirene® MS 20 A Linear Low Density Polyethylene Flexirene MS 20 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 20 A are characterized by optimum low tempe.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 190 °C |
26 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Flexirene® MS 20 U Linear Low Density Polyethylene Flexirene MS 20 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 20 U are characterized by optimum low tempe.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 190 °C |
26 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Flexirene® MS 26 A Linear Low Density Polyethylene Flexirene MS 26 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 26 A are characterized by optimum low tempe.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 260 °C |
26 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Melt Flow | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BFL2000U PC Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
Melt Flow | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXG171R PC (Europe-Africa-Middle East) LEXAN FXG171R is a transparent/translucent high flow grade for special effects colors with a diamond sparkle appearance. Color package may affect performance.This data was supplied by SABIC-IP for t.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 260 °C |
26 g/10 min @Load 4.76 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® B 3225 901510 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 220 °C |
26 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 266 °C |
26 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® IQNH2900 PBT+PC (Asia Pacific) UL94 V-0 Performance with Non-Brominated Flame Retardant. PCR% is up to 12% by using Valox iQ* resin. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 250 °C |
26 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® LF-1030 PC, Unreinforced Anti-Abrasion Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 220 °C |
26 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1014S PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 220 °C |
26 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 220 °C |
26 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1001T PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 230 °C |
26 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 330 °C |
26 g/10 min @Load 4.76 lb, Temperature 626 °F |
ISO 1133 |
Covestro Apec® 1603 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 230 °C |
26 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
ExxonMobil Exxtral™ H1025W Performance Polyolefin Product Description: A polyolefin injection molding compound designed with good flow, cold temperature impact resistance, low CLTE, weatherable mold-in-color and also suitable for painted automotive.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 325 °C |
26 g/10 min @Load 4.76 lb, Temperature 617 °F |
DAM; cm³/10min; ISO 1133 |
DuPont Performance Polymers Zytel® HTN FR52G30BL NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 235 °C |
26 g/10 min @Load 11.0 lb, Temperature 455 °F |
3 min.; ASTM D1238 |
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer Unfilled PA 11 formulated for easy processing. Can be run as a drop-in replacement for other commercially available PA 11 laser sintering powders. Parts produced from PA 850 exhibit outstanding mech.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 190 °C |
26 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform H 4320 Q600 POM Ultraform H4320 Q600 is an extrusion POM high molecular weight grade. This grade enables high extrusion rates with thick-walled product. It also exhibits high thermal stability and a low tendency .. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 250 °C |
26 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
BLUESTAR 101G0 PBT Typical Applications: Appliance, partsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 26 - 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
26 - 34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
AKG Polymers Vision PP PPH TC3004 Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 200 °C |
26 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Total Lacqrene® 2901 Medium Impact Polystyrene
(discontinued **) LACQRENE® 2901 is a very easy flowing, medium impact polystyrene for injection molding. The very high flow of this grade allows for the production of thin wall section or long flow path molding on.. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |