Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
17.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Asia Pacific) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Melt Flow | 17.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
17.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Europe-Africa-Middle East) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 121 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 121 PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 123 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 123R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not .. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific) LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® 221 PC 17.5 MFR, for small, intricate parts. Improved flame retardance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 221 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® 223 PC 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP2JP PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP2R PC Med/High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS2 PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® LI1813R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® LS1 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Low viscosity. UV-stabilized. Transparent colors only. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® LS1 PC (Asia Pacific) Automotive lens applications. Low viscosity. UV-stabilized. Transparent colors only. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East) Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® OQ2220 PC Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Melt Flow | 17.5 g/10 min @Load 5.00 kg, Temperature 266 °C |
17.5 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® XLG2400 PC+PET Low Gloss Xenoy, providing inherent low gloss on almLow Gloss Xenoy, providing inherent low gloss on almost every type of tool surfaces. This grade has excellent low temperature impact, high heat re.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SFX123RU PC SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s.. |