Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 15.5 g/10 min | 15.5 g/10 min | Condition 230/2-8; ASTM D1238 |
Plaskolite Optix® CA-51 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Medium heat resistance and medium flow. |
|||
Melt Flow | 15.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
15.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Melt Flow | 15.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
15.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Melt Flow | 15.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
15.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Melt Flow | 15.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
15.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Nova 8077 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app.. |
|||
Melt Flow | 15.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
15.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min |
Polimeri Europa SINKRAL PD H210/K ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,085-25-16-25 Flame retarded (PBBE free) injection moulding grade, rated UL94-5V at 3.2 mm thick and UL 94V-0 at.. |
|||
Melt Flow | <= 15.5 g/10 min @Load 10.0 kg, Temperature 380 °C |
<= 15.5 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-8168 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM AUT230 PEI (Europe-Africa-Middle East) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 337 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem HTX1010F PEI (Asia Pacific) Higher impact, Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 15.5 g/10 min @Load 5.00 kg, Temperature 300 °C |
15.5 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2956 PPE+PS (Asia Pacific) PPE+PS GF+Mineral Filler total 35% FR V-0 |
|||
Melt Flow | 15.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
15.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM AUT230 PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Melt Flow | 15.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
15.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
Melt Flow | 15.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
15.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
Melt Flow | 15.5 g/10 min @Load 5.00 kg, Temperature 275 °C |
15.5 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry) Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.Information provided by BASF |
|||
Melt Flow | 15.5 g/10 min | 15.5 g/10 min | Condition 230/2-8; ASTM D1238 |
Plaskolite West Optix® CA-51 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Medium heat resistance and medium flow. |
|||
Melt Flow | 15.5 g/10 min | 15.5 g/10 min | Condition G |
Ineos Nova 3510 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Melt Flow | 15.5 g/10 min | 15.5 g/10 min | Condition G |
Ineos Nova 3511 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Melt Flow | 15.5 g/10 min | 15.5 g/10 min | Condition G |
Ineos Nova 5711 High Impact Polystyrene
(discontinued **) High flow, High impact, USP Class VIApplications: Thin wall, Medical, Housewares, ToysProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Inform.. |