Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.7 g/10 min | 1.7 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 7699 BLK Multi-Flex® A 7699 is an acoustic barrier compound for medium density applications . Multi-Flex® TPE compounds are based on Shell Kraton G polymers licensed to Multibase. Multi-Flex TPE contains.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg |
1.7 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Reclair F22020 Polyethylene Butene comonomer based Linear Low Density Polyethylene blow film grade. Reclair F22020 has optimum levels of antioxidants, antiblocking agents, and slip additives. Applications:general purpose, and.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman 1830A Polyethylene
(discontinued **) Polyethylene 1830A is a low density formulation. It is suggested for injection molding applications requiring good stiffness or gloss properties . It us used in applications such as closures.Polyet.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman 1830F Polyethylene
(discontinued **) Polyethylene 1830F is a low-density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat sealing range and.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman 800E Polyethylene
(discontinued **) Polyethylene 800E is used in general-purpose extrusion applications that also require good stress resistance. This formula complies with FDA regulations at 21 CFR177.1520 (c)(2.2) for use in articl.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman Voridian 800P Polyethylene
(discontinued **) General purpose low density formulation used for extrusion coating applications that require good stress resistance. This formula complies with FDA regulations at 21 CFR 177.1520(c)(2.1) for use i.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman E6838-862A Polyethylene
(discontinued **) E6838-862A is a low density formulation suggested for injection molding applications, such as closuresInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemic.. |
|||
Melt Flow | 1.7 g/10 min | 1.7 g/10 min | melt index; ASTM D1238 |
Asahi Kasei Tenac® 2013A Acetal Homopolymer, UV Stabilized
(discontinued **) Similar to 3013A, but higher in molecular weight.Applications: Pipe fittings, rollers, exterior automotive parts.This product is not a part of the standard product line dated 2003. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 8504 BK, 8504 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Low melt index, excellent ESCR, high toughness at low temperatures.Applications: Large chemical storage tanks.Data provided by the manufacturer. |
|||
Melt Flow | 1.7 - 2.3 g/10 min | 1.7 - 2.3 g/10 min | ±12% |
Kazanorgsintez 108-225 Film Grade Composition of High Density Polyethylene Production Method: Based on polyethylene grades 10803-20, 15803-20, 15813-020,17504-006. Application: Designed for packing manufacture for milk and milk products.Information Provided by Kazanorg.. |
|||
Melt Flow | 1.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
M. Holland Company AB105 ABS Features: Medium Flow, High Impact Resistance, Good StiffnessUses: Household Goods, Packaging Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Melt Flow | 1.7 - 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 - 2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PH 0241 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Melt Flow | 1.7 - 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 - 2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PH 0242 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Iran Petrochemical (PCC) SD-0150 Acrylonitrile Butadiene Styrene General Purpose ABS, SD 0150 grade, is a rigid thermoplastic with good processing characteristics. It is a high flow injection molding grade with considerable impact strength and medium heat deflec.. |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
IRPC Polimaxx Polene GP110 Polystyrene APPLICATIONS: EXTRUSION SHEET, HOUSEHOLD PRODUCTS VACUUM SHEET , FOOD PACKAGING, TOY, SANITARY WARE, etc. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos R01A-01 Polypropylene Copolymer, Antistatic An antistated polypropylene random copolymer produced by Ineos utilizing unique catalyst technology. It is designed for blowmolding and extrusion applications and exhibits good stiffness and improv.. |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
Condition G; ASTM D1238 |
Spartech Royalite R21M General Purpose ABS Resin Data provided by the manufacturer. A general-purpose ABS resin with high impact strength, R-21M is a popular choice for a variety of products, from bicycle helmets and carrying cases to portable ta.. |
|||
Melt Flow | 1.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Styron Magnumâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) High Impact, High Heat, Blow Molding ABSInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar®.. |
|||
Melt Flow | 1.7 g/10 min | 1.7 g/10 min | ASTM D1238/E |
Borealis Borstar® HE6067 Black Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6067 is a black, bimodal, co-polymer high density polyethylene (HDPE) compound produced according to the bimodal Borstar process. It is characterized by its balanced properties important .. |
|||
Melt Flow | 1.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
PlastxWorld CEVIAN®-V 420 ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EN1817AA Low Density Polyethylene Westlake Polyethylene EN1817 is a low density formulation suggested for film applications requiring high clarity, good tear and impact strength, good printability and a wide heat-sealing range.Appli.. |
|||
Melt Flow | 1.7 g/10 min @Temperature 230 °C |
1.7 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 2302E Impact Copolymer Polypropylene Impact Copolymer for Extrusion Applications Formolene® 2302E is a low flow, medium impact polypropylene copolymer designed for extrusion applications. It is a barefoot resin with a basic stabilizat.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ UL 00218CC3 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00218CC3 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperature above 240°C (464°F) may cause resin degradation.Availability: Africa & M.. |
|||
Melt Flow | 1.7 g/10 min | 1.7 g/10 min | 190 / 21.6 (HLMI); ASTM D1238 |
ExxonMobil Paxon™ FD60-018 Compression Molding Resin FD60-018 is a very high molecular weight high density polyethylene powder. It exhibits very high impact strength.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 235 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 455 °F |
after drying; ISO 1133 |
Arkema Group Orgalloy® LT 4060 Polyamide Alloy Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Melt Flow | 1.7 g/10 min | 1.7 g/10 min | ASTM D-1238 |
Bapolene® 200B Polyethylene, Film Extrusion Bapolene 200B is a low density polyethylene for blown film applications requiring superior clarity. It complies with US FDA 21CFR177.1520.Applications: General purpose, bakery, flexible, medical an.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 1102 G Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 1.7 - 2.3 g/10 min | 1.7 - 2.3 g/10 min | ±12% |
Kazanorgsintez 108-76 Film Grade Composition of High Density Polyethylene Production Method: Based on polyethylene grades 10803-20, 15803-20, 15813-020,17504-006. Application: Designed for packing manufacture for milk and milk products.Information Provided by Kazanorg.. |